首页> 外国专利> METHOD FOR PRODUCING SILICON-CONTAINING PARTICLES FOR ANODE ACTIVE MATERIAL FOR NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY ANODE MEMBER FOR NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY AND SILICON-CONTAINING PARTICLES FOR ANODE ACTIVE MATERIAL FOR NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY

METHOD FOR PRODUCING SILICON-CONTAINING PARTICLES FOR ANODE ACTIVE MATERIAL FOR NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY ANODE MEMBER FOR NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY AND SILICON-CONTAINING PARTICLES FOR ANODE ACTIVE MATERIAL FOR NON-AQUEOUS ELECTROLYTE SECONDARY BATTERY

机译:非水电解质二次电池的非水电解质二次电池和非硅酸锂二次电池的阳极活性物质的含硅颗粒的制备方法非水电解质二次电池的阳极成员

摘要

In the present invention, silicon-containing particles for a negative electrode active material for a non-aqueous electrolyte secondary battery were prepared by heating the silicon-containing particles obtained by a vapor deposition method under a reducing atmosphere, for example, in a temperature range of 400-1100 ° C. In addition, the silicon-containing particles for a negative electrode active material for a nonaqueous electrolyte secondary battery produced by this production method were made to have a negative electrode active oxygen content for a nonaqueous electrolyte secondary battery of 0.1 to 1.5% by mass. Thereby, when used as a negative electrode active material for a nonaqueous electrolyte secondary battery, it is possible to obtain a nonaqueous electrolyte secondary battery having little volume change during charging and discharging and having excellent initial cycle efficiency and excellent cycle characteristics.
机译:在本发明中,非水电解质二次电池用负极活性物质用含硅粒子是通过在减压气氛下,例如在一定温度范围内对通过蒸镀法得到的含硅粒子进行加热而制备的。另外,通过该制造方法制造的非水电解质二次电池用负极活性物质用含硅粒子的非水电解质二次电池用负极活性氧含量为0.1〜0.1。至1.5质量%。由此,当用作非水电解质二次电池的负极活性物质时,可以得到充放电时的体积变化少,初期循环效率优异,循环特性优异的非水电解质二次电池。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号