Comparative study of Ni, Co, Cu supported on gamma-alumina catalysts for hydrogen production via the glycerol steam reforming reaction

机译:负载于γ-氧化铝催化剂上的甘油,水蒸气重整反应制氢的镍,钴,铜的比较研究

获取原文
获取原文并翻译 | 示例
           

摘要

Catalysts with active phase Ni, Co or Cu supported on gamma-alumina were synthesized at constant loading (8 wt.%) and tested for the glycerol steam reforming reaction (GSR). The synthesized samples, at their calcined and/or their reduced form, were characterized by BET, ICP, XRD, DRS, NH3-TPD, CO2-TPD, TPR and SEM. The carbon deposited on their surface under reaction conditions was characterized by TEM, TPO, TGA and Raman. Catalytic performance for the glycerol steam reforming reaction was studied in order to investigate the effects of reaction temperature on: (i) glycerol total conversion, (ii) glycerol conversion to gaseous products, (iii) hydrogen selectivity and yield, (iv) selectivity of carbonaceous gaseous products, (v) selectivity of liquid products and (vi) molar ratios of H-2/CO and CO/CO2 in the gaseous products' mixture. The stability of all catalysts was also investigated through time on stream experiments. It was concluded that catalytic performance, including liquid products' distribution, depends on the acid-base properties of the materials. Specifically, a drastic drop in the activity of the Ni/Al catalyst was observed, while Co/Al and Cu/Al catalysts deactivate in a slower rate, confirming that coke deposition, associated with dehydration, cracking and polymerization reactions, takes place on the catalyst's surface strong acid sites. (C) 2016 Elsevier B.V. All rights reserved.
机译:以恒定的负载量(8重量%)合成了负载在γ-氧化铝上的具有活性相Ni,Co或Cu的催化剂,并测试了甘油蒸汽重整反应(GSR)。通过BET,ICP,XRD,DRS,NH3-TPD,CO2-TPD,TPR和SEM对合成样品的煅烧和/或还原形式进行表征。在反应条件下沉积在其表面上的碳通过TEM,TPO,TGA和拉曼表征。为了研究反应温度对以下条件的影响,研究了甘油蒸汽重整反应的催化性能:(i)甘油总转化率;(ii)甘油向气态产物的转化率;(iii)氢的选择性和产率;(iv)的选择性碳质气态产物,(v)液态产物的选择性,以及(vi)气态产物混合物中H-2 / CO和CO / CO2的摩尔比。还通过流式实验研究了所有催化剂的稳定性。结论是,包括液体产物分布在内的催化性能取决于材料的酸碱性质。具体而言,观察到Ni / Al催化剂的活性急剧下降,而Co / Al和Cu / Al催化剂以较慢的速度失活,这证实了与脱水,裂化和聚合反应有关的焦炭沉积发生了。催化剂表面的强酸位。 (C)2016 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号