A multi-(amino acid) polymer-hydroxyapatite bone repair material, a supporting-type implant and a preparation method. The repair material is formed by a multi-(amino acid) polymer consisting of ε-aminocaproic acid and other α-amino acids and a modified hydroxyapatite component. For the modified hydroxyapatite component, a medically acceptable calcium salt having a solubility higher than that of hydroxyapatite is used as a modifying component and forms, together with hydroxyapatite, the modified hydroxyapatite; the mass ratio of the calcium salt as the modifying component to the hydroxyapatite is (2-20):(98-80), and the modified hydroxyapatite accounts for 10-70% of the mass of the bone repair material; and the ε-aminocaproic acid in the multi-(amino acid) polymer accounts for 60-99% of the total molar weight of the multi-(amino acid) polymer. Micro-degradation can occur on the surface of the supporting-type implant prepared from the repair material under the action of interstitial fluid, massive calcium/phosphor ions can be quickly released, so that quick healing of bone tissues can be quickly promoted, enough mechanical strength can be stably maintained, and basic requirement for mechanical support in the tissue healing process can be met.
机译:一种多(氨基酸)聚合物-羟基磷灰石骨修复材料,支撑型植入物及其制备方法。该修复材料由由ε-氨基己酸和其他α-氨基酸以及改性的羟基磷灰石组分组成的多(氨基酸)聚合物形成。对于改性的羟基磷灰石组分,将溶解度高于羟基磷灰石的医学上可接受的钙盐用作改性组分,并与羟基磷灰石一起形成改性的羟基磷灰石。作为改性成分的钙盐与羟基磷灰石的质量比为(2-20):(98-80),改性羟基磷灰石占骨修复材料质量的10-70%。聚(氨基酸)聚合物中的ε-氨基己酸占聚(氨基酸)聚合物总分子量的60-99%。在组织液的作用下,由修复材料制成的支撑型植入物的表面会发生微降解,钙/磷离子可以快速释放,从而可以快速促进骨组织的快速愈合,并具有足够的机械性可以稳定地保持强度,并且可以满足组织愈合过程中对机械支撑的基本要求。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号