Iron-oxide hosted copper-gold (IOCG) deposit is a newly recognized raw material for copper recovery. A poor understanding of its hydrometallurgical behavior has limited the development of its commercial practice for copper extraction. In this paper, the leaching behavior of IOCG ore in sulfuric acid medium containing hydrogen peroxide were studied in shaking flask and rolling-ball (RB) vessel. The dissolved copper and iron, pH and oxidation-reduction potential were monitored versus time. It was found that the IOCG ore is more difficult to leach than primary and secondary copper ores. Furthermore, some variables including sulfuric acid dosage, hydrogen peroxide addition and particle sizes were considered and investigated. The similar copper recovery was observed with the variation of the amount of sulfuric acid, and the addition of hydrogen peroxide did not enhance copper yield considerably. Although the higher copper recovery occurred with smaller particle sizes, the highest copper extraction was still not over 40 percent even for -0.02 mm size. The dissolved copper level behavior with time in shaking flask indicates the hindered dissolution is occurring. Moreover, more than 90 percent copper recovery in RB leaching confirmed the existing hindered dissolution in shaking flask. The passivation candidates of elemental sulfur was detected and confirmed by X-ray diffraction further, which were responsible for the low copper yield in shaking flask.
机译:氧化铁基铜金(IOCG)矿床是一种新发现的用于铜回收的原材料。对其湿法冶金行为的了解不足,限制了其铜提取商业实践的发展。本文研究了IOCG矿石在摇瓶和滚球(RB)容器中在含过氧化氢的硫酸介质中的浸出行为。随时间监测溶解的铜和铁,pH和氧化还原电位。已经发现,IOCG矿石比初级和次级铜矿石更难浸出。此外,还考虑并研究了一些变量,包括硫酸用量,过氧化氢的添加量和粒径。随着硫酸量的变化,观察到相似的铜回收率,并且过氧化氢的添加不能显着提高铜的产率。尽管较小的颗粒尺寸会产生较高的铜回收率,但即使-0.02 mm的尺寸,最高的铜提取率仍不超过40%。摇瓶中的溶解铜水平随时间变化表明发生了溶解障碍。此外,RB浸出中超过90%的铜回收率证实了摇瓶中存在的溶解障碍。 X射线衍射进一步检测并确认了元素硫的钝化候选物,这是摇瓶中铜收率低的原因。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号