Metal ductility evaluation by flattening test: The geometry dependence

机译:通过平坦测试的金属延展性评估:几何依赖性

获取原文
获取原文并翻译 | 示例
           

摘要

The reliability of pipes, tubes and liquid tanks (cylinders) is of paramount significance to our life. The typical way to examine the ability of those structures to undergo plastic deformation is to apply a flattening test. In this paper, we used the Gurson-Tvergaard-Needleman damage model and finite element simulations to capture the flattening of a tube made of typical pipe materials. We demonstrated how the tube thickness, radius, and length would affect the critical displacement where tube failure initiates. For flattening with platens, the failure displacement first increases with tube length and reaches a peak value, and it then decreases and converges to a constant value for a particular geometry. The failure initiates at the two edges of short tubes, but shifts to the center in intermediate tubes where the failure displacement maximizes. Failure then always starts from the middle in even longer tubes. In contrast, flattening with indenters exhibits two peaks in the compressible displacement vs. tube length curve. In the end, we proposed effective experimental strategies to obtain the intrinsic ability of tubes under plastic deformation. The results reported here could be employed to characterize the mechanical properties of materials for pipes, tubes and tanks, and they could also be applied to guide the engineering design of such structures.
机译:管道,管和液体罐(气缸)的可靠性对我们的生活具有最重要的意义。检查这些结构进行塑性变形的能力的典型方式是施加平坦化测试。在本文中,我们使用了Gurson-Tvergaard-Calleleman损坏模型和有限元模拟,以捕获由典型管道材料制成的管的扁平化。我们证明了管厚度,半径和长度如何影响管衰竭启动的临界位移。为了用压板扁平化,故障位移首先用管长度增加并达到峰值,然后达到峰值,然后将其收敛于特定几何形状的恒定值。故障在短管的两个边缘发起,但在中间管中转移到失效位移最大化的中间管中。然后,失败始终从中间开始在更长的管中。相反,用压痕的平坦化在可压缩位移与管长度曲线中呈现两个峰。最后,我们提出了有效的实验策略,以获得塑性变形下管的内在能力。这里报道的结果可以用于表征管道,管和罐材料的机械性能,并且还可以应用于引导这种结构的工程设计。

著录项

  • 来源
  • 作者单位

    Beijing Jiaotong Univ Engn Res Ctr Struct Reliabil &

    Operat Measurement Minist Educ Beijing 100044 Peoples R China;

    Beijing Jiaotong Univ Engn Res Ctr Struct Reliabil &

    Operat Measurement Minist Educ Beijing 100044 Peoples R China;

    Chinese Acad Sci Inst Mech State Key Lab Nonlinear Mech LNM Beijing 100190 Peoples R China;

    Beijing Jiaotong Univ Engn Res Ctr Struct Reliabil &

    Operat Measurement Minist Educ Beijing 100044 Peoples R China;

    Chinese Acad Sci Key Lab Nucl Mat &

    Safety Assessment Inst Met Res Shenyang 110016 Liaoning Peoples R China;

    Chinese Acad Sci Key Lab Nucl Mat &

    Safety Assessment Inst Met Res Shenyang 110016 Liaoning Peoples R China;

    Beijing Jiaotong Univ Engn Res Ctr Struct Reliabil &

    Operat Measurement Minist Educ Beijing 100044 Peoples R China;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类 蒸汽动力工程;
  • 关键词

    Flattening test; Plastic deformability; Gerson-Tvergaard-Needleman model; Failure; Finite element analysis;

    机译:扁平化试验;塑料可变形性;Gerson-Tvergaard-Constleman模型;失败;有限元分析;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号