The present controlled in vitro experiment evaluated the dissolution kinetics of titanium (Ti), aluminum (Al) and vanadium (V). Titanium alloy (Ti90Al6V4) dental implants were inserted in 1.8 ml sterile tubes, containing equal volumes of NaCl 0.9% (w/v) and human serum. Metallic elements released by the atomic process of corrosion were measured at pH 7.2 and 37 C by atomic absorption spectrophotometer at 1, 3, 6, 9, 15, 21, 27, 33, 42, 51, 60, 69, 78, 87 and 96 days. Ti dissolution averaged 16+/-5 ng/cm2/day and 1565 ng/cm2 over the experimental period. Al dissolution was stable at 9+/-5 ng/cm2/day and averaged 945 ng/cm2 over the 96-day period. V dissolution was stable at 0.15+/-0.18 ng/cm2/day after the sixth day of incubation and averaged 42 ng/cm2 over the 96-day period. Major disparities in atomic dissolution were detected among implants. No local or systemic reaction to titanium has been documented. In contrast, 4% toxic V and 6% Al may suffice to elicit local and systemic reactions or inhibit cellular proliferation and differentiation.
机译:本对照体外实验评估了钛(Ti),铝(Al)和钒(V)的溶解动力学。将钛合金(Ti90Al6V4)牙科植入物插入1.8 ml无菌管中,该管中含有等体积的0.9%(w / v)的NaCl和人血清。通过原子吸收分光光度计在1、3、6、9、15、21、27、33、42、51、60、69、78、87和96天在整个实验期间,钛的平均溶解度为16 +/- 5 ng / cm2 /天和1565 ng / cm2。铝的溶出稳定在9 +/- 5 ng / cm2 /天,在96天期间平均为945 ng / cm2。在培养的第六天后,V溶出稳定在0.15 +/- 0.18 ng / cm2 /天,在96天的时间内平均为42 ng / cm2。在植入物中发现原子溶解的主要差异。没有关于钛的局部或全身反应的文献。相比之下,4%的毒性V和6%的Al可能足以引起局部和全身反应或抑制细胞增殖和分化。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号