Preparation of Co_(0.5)Zn_(0.5)Fe_2O_4 and Co_(0.5)Mn_(0.5)Fe_2O_4 Nano ferrites by Coprecipitation Method

机译:通过共沉淀法制制备CO_(0.5)Zn_(0.5)Zn_(0.5)Fe_2O_4和CO_(0.5)Fe_2O_4纳米铁氧体

获取原文

摘要

Nanoparticles of Cobalt-zinc ferrite (Co_(0.5)Zn_(0.5)Fe_2O_4) and Cobalt-manganese ferrite (Co_(0.5)Mn_(0.5)Fe_2O_4) have been synthesized at room temperature by co-precipitation method with and without calcination process. Starting materials for preparation of nano oxides were Co(NO_3)_2·6H_2O, ZnCl_2, Fe(NO_3)_3·9H_2O and Mn(NO_3)_2·4H_2O. These salats were mixed in stoichiometric amounts and precipitated with sodium hydroxide. Synthesised materials are confirmed by XRD and SEM analysis. The FTIR spectra of nano oxides have been analyzed in the frequency range of 400-4000 cm~(-1).
机译:通过在室温下通过具有和无煅烧过程的共沉淀法在室温下合成了钴 - 锌铁氧体(CO_(0.5)Zn_(0.5)Zn_(0.5)Fe_2O_4)和钴 - 锰铁素体(CO_(0.5)MN_(0.5)FE_2O_4)。用于制备纳米氧化物的原料是CO(NO_3)_2·6H_2O,ZnCl_2,Fe(NO_3)_3·9H_2O和Mn(NO_3)_2·4H_2O。将这些盐在化学计量的量中混合并用氢氧化钠沉淀。通过XRD和SEM分析确认合成材料。在400-4000cm〜(-1)的频率范围内分析了纳米氧化物的FTIR光谱。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号