A pipe for a steam turbine is formed of a centrifugal casting material to achieve resistance against higher temperatures and improve reliability of the pipe by employing, as a pipe material, a centrifugal casting material normalized to contain uniform and finer crystal grains. The centrifugal casting material is made of steel having a columnar structure in the radial direction with the crystal grain size number of 5 or more in a plane perpendicular to the radial direction. The steel includes 0.05-0.5% by mass C, not more than 1.0% Si, 0.05-1.5% Mn, 0.01-2.5% Ni, 8.0-13.0% Cr, 0.05-2.5% Mo, not more than 3.0% W, 0.05-0.35% V, 0.01-0.5% Nb, not more than 5% Co, 0.01-0.1% N, not more than 0.03% B, and not more than 0.05% Al.
机译:用于蒸汽涡轮机的管由离心铸造材料形成,以通过使用标准化为包含均匀且更细的晶粒的离心铸造材料作为管道材料来实现耐高温性并提高管的可靠性。离心铸造材料由在径向上具有柱状组织的钢制成,在垂直于径向的平面中晶粒尺寸数为5以上。该钢包括按质量计0.05-0.5%的C,不超过1.0%的Si,0.05-1.5%的Mn,0.01-2.5%的Ni,8.0-13.0%的Cr,0.05-2.5%的Mo,不超过3.0%的W,0.05 -0.35%V,0.01-0.5%Nb,不超过5%Co,0.01-0.1%N,不超过0.03%B和不超过0.05%Al。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号