PROBLEM TO BE SOLVED: To provide a pipe used for a steam turbine, which employs a centrifugal-cast material having crystal grains uniformly refined, and consequently can raise the temperature of the pipe higher and enhance the reliability of the pipe; a manufacturing method therefor; and a main steam pipe for the steam turbine, a reheating pipe and a steam turbine power plant which use the pipe for the steam turbine.;SOLUTION: The pipe for the steam turbine is made from a martensitic steel material which contains columnar grains that orient in a diametric direction and have crystal grain size numbers of 5 or more in a plane perpendicular to the diametric direction; is manufactured by a centrifugal casting method; and comprises, by mass, 0.05-0.5% C, 1.0% or less Si, 0.05-1.5% Mn, 0.01-2.5% Ni, 8.0-13.0% Cr, 0.05-2.5% Mo, 3.0% or less W, 0.05-0.35% V, 0.01-0.5% Nb, 5% or less Co, 0.01-0.1% N, 0.03% or less B, 0.05% or less Al, and the balance iron with unavoidable impurities.;COPYRIGHT: (C)2007,JPO&INPIT
机译:解决的问题:提供一种用于蒸汽涡轮机的管道,该管道采用具有均匀细化的晶粒的离心铸造材料,因此可以提高管道的温度并提高管道的可靠性。其制造方法;解决方案:蒸汽轮机的管道由马氏体钢材料制成,其中包含定向的圆柱状晶粒。在垂直于直径方向的平面上具有5或更大的晶粒尺寸数;通过离心铸造法制造;且按质量计包含0.05-0.5%C,1.0%以下Si,0.05-1.5%Mn,0.01-2.5%Ni,8.0-13.0%Cr,0.05-2.5%Mo,3.0%以下W,0.05- 0.35%V,0.01-0.5%Nb,5%或更少的Co,0.01-0.1%N,0.03%或更少的B,0.05%或更少的Al和余量的铁具有不可避免的杂质。;版权所有:(C)2007日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号