A PROCESS FOR MAKING IRON TANNED LEATHER USING NATURAL POLYSACCHARIDE

机译:利用天然多糖制作铁鞣革的方法

摘要

At present, the awareness among the public is becoming more about the pollution related problems associated with chrome tanning method, which is a versatile tanning system often stated that about 85-90% of all leathers produced are chrome tanned. Iron salts have been reported to be inexpensive and non-polluting with interesting tanning abilities. The previous attempts shows that even with proper masking salts a solo iron tannage can be achieved a shrinkage temperature of 80-97°C. In this connection, arabinogalactan protein complex, which is a complex natural polysaccharide, is employed as masking agent along with ferric sulphate, tartarate, and phthalate as chelating ligands. The resultant leathers show a shrinkage temperature of 108 -110°C.
机译:目前,公众越来越意识到与铬鞣制法有关的与污染有关的问题,铬制革是一种多用途的鞣制系统,通常说出所生产的皮革中约有85-90%是铬鞣制的。据报道,铁盐便宜且无污染且具有令人愉悦的鞣制能力。先前的尝试表明,即使使用适当的掩蔽盐,单铁鞣制也可以实现80-97°C的收缩温度。在这方面,阿拉伯半乳聚糖蛋白复合物是一种复杂的天然多糖,与硫酸铁,酒石酸盐和邻苯二甲酸酯作为螯合配体一起用作掩蔽剂。所得皮革的收缩温度为108 -110℃。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号