首页> 外国专利> A method to measure fireside corrosion resistance of boiler components of ultra super critical boiler using indian coal ash or flyash at simulated boiler condition'

A method to measure fireside corrosion resistance of boiler components of ultra super critical boiler using indian coal ash or flyash at simulated boiler condition'

机译:在模拟锅炉条件下用印度煤灰或粉煤灰测量超超临界锅炉锅炉部件耐火侧腐蚀的方法”

摘要

The invention relates to A method to measure fireside corrosion resistance of boiler components of ultra super critical boiler using Indian coal ash or flyash at simulated boiler condition, comprising the steps of: preparing a plurality of specimen formed of a base material corresponding to that of the boiler components; preparing a plurality samples of weld corresponding to that used in said boiler components; determining individually initial weight including dimension of all the base material specimen including that of the weld samples; preparing a plurality of mixtures formed of coal ash/ fly ash, alkali sulfate, and sodium chloride, each of said plurality of mixtures being formed of different composition of said constituent material, setting a timer and activating a thermocouple in the boiler simulation and placing the specimen/samples inside the simulator, the specimen/samples being covered with one of said plurality mixture; raising the temperature in stages within the simulator corresponding to that of resistance tubular furnace and allowing soaking of the specimen/samples for predetermined period and recording simultaneously the temperature through the thermocouple; taking out the specimen/samples after completion of soaking from the simulator and cleaning with acetone in an ultrasonic cleaning machine; washing with water and drying the cleaned samples/specimen by a drying machine; and measuring the weight and dimension of each specimen/sample to determine the corrosion loss.
机译:本发明涉及一种在模拟锅炉条件下使用印度粉煤灰或粉煤灰测量超超临界锅炉锅炉部件耐火腐蚀性能的方法,该方法包括以下步骤:制备多个与基体材料相对应的由基体材料形成的试样。锅炉部件;制备与所述锅炉部件中使用的焊缝相对应的多个焊缝样品;分别确定包括所有基础材料试样的尺寸在内的初始重量,包括焊接样品的尺寸;制备由煤灰/飞灰,碱式硫酸盐和氯化钠形成的多种混合物,所述多种混合物中的每一种均由所述组成材料的不同组成形成,设置计时器并在锅炉模拟中激活热电偶并将其放置模拟器内的样品/样品,所述样品/样品被所述多种混合物之一覆盖;在模拟机内分阶段升高与电阻管式炉相对应的温度,并允许将样本/样品浸泡预定的时间,并通过热电偶同时记录温度;从模拟器中浸透完成后取出样品/样品,并在超声波清洗机中用丙酮清洗;用水洗涤并通过干燥机干燥清洁的样品/样品;测量每个样品/样品的重量和尺寸,以确定腐蚀损失。

著录项

  • 公开/公告号IN2013KO01065A

    专利类型

  • 公开/公告日2015-03-20

    原文格式PDF

  • 申请/专利权人

    申请/专利号IN1065/KOL/2013

  • 发明设计人 DR MRS NAGALAKSHMI RAMESH;

    申请日2013-09-13

  • 分类号B08B3;

  • 国家 IN

  • 入库时间 2022-08-21 15:14:55