Thickener comprising at least one associative polymers based on monomers and are prepared by inverse emulsion polymerization of

机译:增稠剂包括至少一种基于单体的缔合聚合物,并通过反相乳液聚合制备。

摘要

1. A thickener, which may be prepared by a process characterized in that the polymer is obtained by inverse emulsion polimerizatsiia) at least one water-soluble, ethylenically unsaturated monomer comprising at least one anionic monomer and / or at least one nonionic monomer, b) at least one ethylenically unsaturated associative monomer, c) optionally at least one crosslinking agent, d) optionally at least one chain transfer agent, the m mperatura during the inverse emulsion polymerization is kept constant and is at least 40 ° C, and after closure of the inverse emulsion polymerization is carried out addition of an activator to give a thickener and wherein the thickener comprises at least one activator, and the activator is a surfactant. 2. Thickener according to Claim. 1, characterized in that the temperature during the inverse emulsion polymerization of 50-90 ° C.3. Thickener according to Claim. 1, characterized in that after the inverse emulsion polymerization and before addition of the activator is distilled off at least a partial amount of water and at least a partial amount of low boiling components fazy.4 oil. Thickener according to Claim. 1 or 2, characterized in that the method is based on the LDP technology (technology of liquid dispersion polymers) .5. Thickener according to Claim. 1 or 2, characterized in that the inverse emulsion polymerization of component b) is added to the oil fazu.6. Thickener according to Claim. 1 or 2, characterized in that the activator selecting
机译:1.一种增稠剂,其可以通过以下方法制备,其特征在于,所述聚合物是通过反相乳液聚合获得的)至少一种水溶性的烯键式不饱和单体,其包含至少一种阴离子单体和/或至少一种非离子单体,b )至少一种烯键式不饱和缔合单体,c)任选地至少一种交联剂,d)任选地至少一种链转移剂,在反相乳液聚合过程中,mperatura保持恒定且至少40°C,并且在封闭后乳液聚合的逆反应是通过加入活化剂进行的,得到增稠剂,其中该增稠剂包括至少一种活化剂,并且该活化剂是表面活性剂。 2.根据权利要求1的增稠剂。 1,特征在于反相乳液聚合过程中的温度为50-90°C.3。根据权利要求1的增稠剂。 1,特征在于,在反相乳液聚合之后并且在添加活化剂之前,蒸馏出至少一部分水和至少一部分低沸点组分fazy.4油。根据权利要求1的增稠剂。 1或2,其特征在于该方法基于LDP技术(液体分散聚合物技术).5。根据权利要求1的增稠剂。 1或2,其特征在于将组分b)的反相乳液聚合加入油fazu.6中。根据权利要求1的增稠剂。 1或2,其特征在于活化剂选择

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号