METHOD FOR EXTRACTING BASE AND PRECIOUS METALS BY A PRE- TREATMENT THAT LEADS TO SOLUBILISATION OF THE REFRACTORY MATRICES THEREOF

机译:一种通过预处理来提取基础和贵金属的方法,可导致其耐火材料的溶解

摘要

The present invention relates to a method for extracting base and precious metals, all contained in refractory minerals, using aqueous media. The aim is to replace the current “flotation/smelting”-method for extracting minerals in Chilean and global mining or classical leaching with a method comprising a simple and robust pre-treatment that leads to solubilisation of the refractory matrices thereof. The method consists of mixing the mineral (Cu2S, CuS,CuFeS2, Cu5FeS4, FeS2, FeAsS.NiS, (Ni,Fe)xSy), ground to an appropriate size (2.5 centimetres), with a specific dose of solid reagent in a rotary agglomeration drum and then adding slightly acidified water to obtain a defined water content (5-8%) depending on the type of gangue contained in the metal-containing solid, thereby forming an agglomerate that will form a heap, which is subsequently allowed to stand for a period of several days (20-60 days), during which the conditions required to transform the refractory matrix into a highly soluble solid will be generated. Finally, appropriately regulated irrigation is applied, thus resulting in extraction of the metal by simple aqueous washing. In essence, the method achieves maximum transformation of the original refractory mineral into a highly soluble solid salt during a step prior to the conventional leaching process. Thus, the metal will be contained in a solid with a much higher solubility than the original matrix, therefore the dissolution thereof will be faster, more efficient and require a minimal use of consumables and reagents.
机译:本发明涉及一种利用含水介质提取难熔矿物中所含的贱金属和贵金属的方法。目的是用一种方法进行替代,以取代目前的“浮选/冶炼”方法,该方法用于在智利和全球采矿或经典浸出中提取矿物,该方法包括一种简单而稳健的预处理方法,从而可使其难熔基质溶解。该方法包括将矿物(Cu2S,CuS,CuFeS2,Cu5FeS4,FeS2,FeAsS.NiS,(Ni,Fe)xSy)研磨成合适的大小(2.5厘米),然后将特定剂量的固体试剂在旋转仪中混合。结块转鼓,然后根据含金属固体中脉石的类型,添加略微酸化的水以获得规定的水分含量(5-8%),从而形成附聚物,该附聚物将形成堆积,随后使其静置持续几天(20-60天),在此期间,将产生将耐火基质转变成高度可溶固体所需的条件。最后,进行适当调节的灌溉,从而通过简单的水洗就可提取金属。本质上,该方法在传统浸出工艺之前的步骤中实现了将原始耐火矿物最大程度地转化为高可溶性固体盐的过程。因此,金属将以比原始基质高得多的溶解度包含在固体中,因此其溶解将更快,更有效并且需要消耗的消耗品和试剂最少。

著录项

  • 公开/公告号US2020224291A1

    专利类型

  • 公开/公告日2020-07-16

    原文格式PDF

  • 申请/专利权人 EDUARDO LUIS PATINO MARTINEZ;

    申请/专利号US201816628966

  • 发明设计人 EDUARDO LUIS PATINO MARTINEZ;

    申请日2018-09-05

  • 分类号C22B11/08;C22B3/08;C22B11/06;

  • 国家 US

  • 入库时间 2022-08-21 11:25:50

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号