首页> 外文期刊>Solid state sciences >Mechanochemical synthesis of gamma-Bi_2O_3
【24h】

Mechanochemical synthesis of gamma-Bi_2O_3

机译:机械化学合成γ-Bi_2O_3

获取原文
获取原文并翻译 | 示例
           

摘要

A series of gamma-Bi_O_2 phases doped with Zn, Si, Pb and Fe was prepared by mechanochemical treatment of corresponding oxide mixtures with a nominal composition 6Bi_2O_3 centre dot MO_x (MO_x = ZnO, SiO_2, PbO) and 12Bi_2O_3 centre dot Fe_2O_3 using high-energy ball mill. The products are characterized by X-ray powder diffraction technique. Influence of milling conditions: milling time from 5 min to 10 h, milling medium (steel or ZrO_2) and injected mechanical power on unit-cell parameters and crystallinity of products, as well as on reaction kinetics are investigated and discussed.
机译:通过机械化学处理标称成分为6Bi_2O_3中心点MO_x(MO_x = ZnO,SiO_2,PbO)和12Bi_2O_3中心点Fe_2O_3的相应氧化物混合物进行机械化学处理,制备了一系列掺杂Zn,Si,Pb和Fe的gamma-Bi_O_2相。能量球磨机。产品通过X射线粉末衍射技术表征。研磨条件的影响:研究和讨论了研磨时间(从5分钟到10小时),研磨介质(钢或ZrO_2)和注入的机械功率对晶胞参数和产物结晶度以及反应动力学的影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号