Fatigue behavior of deep rolled Al-Mg-Si-Cu alloy at elevated temperature

机译:深轧Al-Mg-Si-Cu合金在高温下的疲劳行为

获取原文
获取原文并翻译 | 示例
           

摘要

A mechanical surface treatment (deep rolling) was applied at room temperature for the aluminium wrought alloy AA6110-T6 (Al-Mg-Si-Cu). The cyclic deformation behavior and s curves of deep rolled AA6110-T6 were investigated by stress-controlled fatigue tests at elevated temperatures up to 250 deg C and compared to the polished condition as a reference. The effect of deep rolling on the fatigue lifetime and residual stresses under high-loading and/or elevated-temperature conditions are discussed.
机译:在室温下对铝锻造合金AA6110-T6(Al-Mg-Si-Cu)进行了机械表面处理(深轧)。通过在高达250摄氏度的高温下进行应力控制疲劳试验,研究了深轧AA6110-T6的循环变形行为和s / n曲线,并与抛光条件进行了比较。讨论了在高负荷和/或高温条件下深轧对疲劳寿命和残余应力的影响。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号