With the continuous depletion of high-grade titanium ores anil the increasing demand for titanium dioxide, the low-grade titanium sand has become an important source for the production of ilmenite concentrate; however, the large-scale utilization of the sand is disappointedly scarce, due to its leanness in valuable minerals and insufficient methods available to handle such low-grade sands. A typically low-grade titanium sand was first ground and then processed by low-intensity magnetic separation (LMS) and high gradient magnetic separation (HGMS) to recover litanomagnetite and ilmenite, respectively; as the TiO_2 grade of the sand is low, the primary treatment of the sand by magnetic separations is effective, with 78.45% by mass weight of the sand discarded as tailings. The primary titanomagnctite concentrate was further ground and liberated to obtain a high-grade titano-magnetite concentrate through LMS reconcentrat'wn; the primary ilmenite concentrate was separated with spirals to remove the sterile limonite and magnetic gangucs, and its concentrate was ground and liberated to achieve a high-grade ilmenite concentrate through HGMS refining. This novel process achieved an effective processing of the sand and obtained a high-grade ilmenite concentrate assaying 46.30% TiO_ with a high recovery of 57.88%, and a by-product of litanomagnetite concentrate assaying as high as 54.17% Fe.
机译:随着高品位钛矿石的不断消耗和对二氧化钛需求的增加,低品位钛砂已成为钛铁矿精矿生产的重要来源。然而,由于其稀有有价值的矿物质和处理此类低品位砂石的方法不足,令人失望的是,砂石的大规模利用令人失望。首先将典型的低品位钛砂磨碎,然后通过低强度磁选(LMS)和高梯度磁选(HGMS)进行处理,分别回收钛磁铁矿和钛铁矿。由于砂的TiO_2品位低,通过磁选对砂进行初步处理是有效的,按质量计有78.45%的砂被作为尾渣丢弃。进一步对初生的钛磁铁矿精矿进行研磨和释放,以通过LMS浓缩法获得高级钛磁铁矿精矿。用螺旋分离方法分离初级钛铁精矿以除去无菌褐铁矿和磁性神经节,然后将其精磨并释放,通过HGMS精制获得高级钛铁精矿。这种新颖的方法有效地处理了沙子,并获得了含量为46.30%TiO_的高品位钛铁矿精矿,回收率高达57.88%,而副磁铁矿精矿的Fe含量高达54.17%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号