The objectives of this study were to investigate the effectiveness of a compliance method for analyzing the fatigue crack growth of GLARE3 fiber/metal laminates. The materials tested were GLARE3-5/4 (2.6 mm thick) and GLARE3-3/2 (1.4 mm thick). Centrally notched specimens with two kinds of notch length and two kinds of fiber orientation were fatigue tested under constant amplitude loading. The expression of the experimental stress intensity factor, K_(exp), for the 2024-T3 aluminum-alloy layers of a GLARE3 is formulated and K_(exp) were obtained from the relationship between crack length and specimen compliance. The test results clarified the following: (1) da/dN-DELTA K_(exp) relationships roughly show the linear relationship independent of the maximum stress level, specimen thickness, notch length, and fiber orientations, (2) the da/dN- DELTA K_(exp) relationships approximately agree with the linear part and its extension of Paris-Erdogan's law obtained for the da/dN- DELTA K relationship of the 2024-T3 aluminum-alloy, (3) the compliance method is effective for analyzing fatigue crack growth in GLARE3 laminates.
机译:这项研究的目的是调查柔韧性方法用于分析GLARE3纤维/金属层压板疲劳裂纹扩展的有效性。测试的材料为GLARE3-5 / 4(2.6毫米厚)和GLARE3-3 / 2(1.4毫米厚)。在恒定振幅载荷下对具有两种切口长度和两种纤维取向的中央切口试样进行了疲劳测试。公式化了GLARE3的2024-T3铝合金层的实验应力强度因子K_(exp)的表达式,并根据裂纹长度和试样柔度之间的关系获得了K_(exp)。测试结果阐明了以下几点:(1)da / dN-DELTA K_(exp)关系大致显示出与最大应力水平,样品厚度,缺口长度和纤维取向无关的线性关系,(2)da / dN- DELTA K_(exp)关系与2024-T3铝合金的da / dN-DELTA K关系获得的Paris-Erdogan定律的线性部分及其扩展近似一致,(3)柔度法对于分析疲劳是有效的GLARE3层压板的裂纹扩展。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号