首页> 外文期刊>Journal of Adhesion Science and Technology: The International Journal of Theoredtical and Basic Aspects of Adhesion Science and Its Applications in All Areas of Technology >Influence of silicoating, etching and heated glaze treatment on the surface of Y-TZP and its impact on bonding with veneering ceramic
【24h】

Influence of silicoating, etching and heated glaze treatment on the surface of Y-TZP and its impact on bonding with veneering ceramic

机译:硅化,蚀刻和加热釉料处理对Y-TZP表面的影响及其对嵌合陶瓷粘接的影响

获取原文
获取原文并翻译 | 示例
           

摘要

The study aimed to investigate the influence of surface treatments of Y-TZP on its topography and their impact on shear bond strength (SBS) of Y-TZP to veneering porcelain. Thirty-four zirconia cubes (Cercon) (10 x 10 x 10 mm(3)) were divided randomly into 3 groups (n = 11) according to the different surface treatments, Silica Coating (SC); Hot Solution Etching (HE); and Heat Treatment after porcelain glaze and powder application (GP). Porcelain application (IPs e.max) was performed after surface treatment using a standardized technique. Porcelain application (Ceramco-3) was also performed on 10 metal cubes (I BOND 2) as controls (MC). Specimens were subjected to thermocycling (5-55 degrees C, 20,000 cycles) followed by SBS testing in a universal testing machine. Surface topography was assessed by scanning electron microscopy and surface roughness (Image J). SC developed significantly higher SBS (42.10 +/- 5.84 MPa) of Y-TZP to veneering ceramics compared to treatment by HE (24.0 +/- 6.4 MPa), GP (23.30 +/- 4.72), and the MC (29.3 +/- 5.4 MPa) control (p 0.05). SBS among HE, GP and MC specimens was comparable (p 0.05). Y-TZP specimens treated with SC and HE showed high surface roughness compared to GP. Silicoating of Y-TZP prior to veneering can potentially reduce the high failure rates of zirconia-based restorations by enhancing the chemical bond between the core and the veneer materials.
机译:该研究旨在探讨Y-TZP表面处理对其地形的影响及其对辅助瓷器剪切粘合强度(SBS)的影响。根据不同的表面处理,二氧化硅涂层(SC)随机将三十四个氧化锆立方体(10×10×10mm(3))随机分成3组(n = 11);热解蚀刻(他);和瓷釉和粉末施用后的热处理(GP)。使用标准化技术在表面处理后进行瓷器应用(IPS E.MAX)。瓷器施用(Ceramco-3)也以10个金属立方体(I键2)为对照(MC)进行。对试样进行热环(5-55℃,20,000个循环),然后在通用试验机中进行SBS测试。通过扫描电子显微镜和表面粗糙度评估表面形貌(图像J)。与HE(24.0 +/- 6.4MPa),GP(23.30 +/- 4.72)和MC(29.3 + / -5.4MPa)控制(P <0.05)。他,GP和MC标本中的SBS相当(P&GT; 0.05)。用SC处理的Y-TZP样品,与GP相比,他表现出高表面粗糙度。在嵌体之前Y-TZP的硅化可以通过增强芯和胶合材料之间的化学键来潜在地降低基于氧化锆的修复的高衰竭率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号