Epoxy composite reinforced with three-dimensional polyimide fiber felt: Fabrication and tribological properties investigation

机译:三维聚酰亚胺纤维毡增强的环氧复合材料的制备和摩擦学性能研究

获取原文
获取原文并翻译 | 示例
           

摘要

Novel epoxy (EP) composite reinforced with three-dimensional (3D) polyimide (PI) fiber felt (PI3D/EP) is first fabricated by vacuum assisted resin transfer molding. The tribological behaviors of pure EP and PI3D/EP composite under dry sliding and water lubricated condition are comparatively studied. Results indicate that both wear rates and friction coefficients of PI3D/EP composite are lower than those of pure EP. The wear resistance of PI3D/EP composite is 9.8 times higher than that of pure EP under dry sliding of 1.5 MPa and 0.76 ms(-1) while a 27-fold increase is achieved under water lubricated condition. The wear mechanisms of PI3D/EP composite are investigated based on tribological testing results and scanning electron microscopy observations. The PI fiber felt provides strong 3D structure supports to sustain most of the loads on the composite, improving the mechanical and tribological properties significantly. (c) 2016 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2016, 133, 44160.
机译:首先通过真空辅助树脂传递模塑法制造了用三维(3D)聚酰亚胺(PI)纤维毡(PI3D / EP)增强的新型环氧(EP)复合材料。比较研究了纯EP和PI3D / EP复合材料在干滑和水润滑条件下的摩擦学行为。结果表明,PI3D / EP复合材料的磨损率和摩擦系数均低于纯EP。在1.5 MPa和0.76 ms(-1)的干滑下,PI3D / EP复合材料的耐磨性是纯EP的9.8倍,而在水润滑条件下的耐磨性增加了27倍。基于摩擦学测试结果和扫描电镜观察,研究了PI3D / EP复合材料的磨损机理。 PI纤维毡提供了强大的3D结构支撑,可承受复合材料上的大部分载荷,从而显着改善了机械和摩擦学性能。 (c)2016 Wiley Periodicals,Inc. J. Appl。 Polym。科学2016,133,44160。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号