The fatigue test of the movement transmission member was done. 1) The life of SUS 304 wire rope is put off by the surface treatment. 2) There are no relations in the stress amplitude, and a crack causing SUS 304 endless belt from the welded section, and it is ruptured. 3) When it is compared with the steel, the fatigue limit ratio of amorphous is a low value of 0.16. 4) The fatigue limit of the Zn coating stainless steel wire rope is 200 N/mm{sup}2 with the tension 2 N, 310N mm{sup}2 with 3N.
机译:对运动传递部件进行了疲劳试验。 1)表面处理延缓了SUS 304钢丝绳的使用寿命。 2)应力振幅没有关系,从焊接部位产生裂纹导致SUS 304环形带断裂。 3)当与钢比较时,非晶态的疲劳极限比为0.16的低值。 4)镀锌不锈钢钢丝绳的疲劳极限为200 N / mm {sup} 2,张力为2 N,310N mm {sup} 2,张力为3N。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号