The forming limit diagrams ( FLD) of AZ31B magnesium, alloy sheet were tested by means of the electro etching grid method based on the forming experiment of magnesium alloy sheet carried out with a BCS-30 D sheet forming testing machine and the strain testing analysis made with an advanced ASAME automatic strain measuring system.. Experiments show that, at room temperature , the mechanical properties and deep drawing performance of AZ31B cold-rolled magnesium alloy sheet were so poor that it failed to lest the forming limit diagrams without an ideal forming and processing capacity, while the hoi-rolled magnesium alloy sheet was of a little better plasticity and forming performance after testing its forming limit diagrams . It can be concluded that the testing of the forming limit curves ( FLC) offers the theoretical foundation for the drawing of the deep drawing and forming process of magnesium alloy sheet.
机译:基于BCS-30 D薄板成型试验机对镁合金薄板的成型实验,通过电蚀刻网格法,对AZ31B镁薄板的成形极限图(FLD)进行了测试,并进行了应变试验分析。实验表明,在室温下,AZ31B冷轧镁合金薄板的机械性能和深冲性能很差,以至于没有理想的成形和成形条件就无法避免成形极限图的产生。在测试其成形极限图后,海轧镁合金薄板具有更好的可塑性和成形性能。可以得出结论,成形极限曲线(FLC)的测试为镁合金薄板的深冲和成形工艺提供了理论依据。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号