Analysis of severely fractured glenoid components: clinical consequences of biomechanics, design, and materials selection on implant performance

机译:关节盂严重骨折的分析:生物力学,设计和材料选择对植入物性能的临床影响

获取原文
获取原文并翻译 | 示例
           

摘要

Background: The longevity of total shoulder replacement is primarily limited by the performance of the ultrahigh-molecular-weight polyethylene (UHMWPE) glenoid component in vivo. Variations in glenoid design (conformity, thickness), biomechanics (joint kinematics), and UHMWPE material selection (sterilization, cross-linking) distinguish total shoulder replacements from hip and knee arthroplasty devices. These variables can lead to severe mechanical failures, including gross fracture.
机译:背景:全肩关节置换术的寿命主要受到体内超高分子量聚乙烯(UHMWPE)关节盂部件的性能限制。关节盂设计(适形性,厚度),生物力学(关节运动学)和UHMWPE材料选择(灭菌,交联)的变化将髋关节和膝关节置换术的总肩关节置换区分开。这些变量可能导致严重的机械故障,包括严重断裂。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号