Extraction of metals from saprolitic laterite ore through pressure hydrochloric-acid selective leaching

机译:通过加压盐酸选择性浸出从腐泥红土矿石中提取金属

获取原文
获取原文并翻译 | 示例
           

摘要

In this study, pressure hydrochloric-add selective leaching was used to leach Ni and Co from saprolitic laterite ore on the basis of potential-pH diagrams constructed for Fe-Si-Cl-H2O and Ni-Si-Cl-H2O systems. The leaching of Ni, Co, Mg, Mn, and Fe was investigated under various conditions. The results showed that the optimal output was obtained under the following conditions: leaching temperature of 150 degrees C, HCl concentration of 350 g/L, liquid to solid ratio (I/s) of 1.0, and leaching time of 90 min. The saprolitic laterite and leached residue were characterized via X-ray diffraction analysis, infrared spectrometry, and mineral liberation analysis. The related acid leaching mechanism was analyzed based on the results, and the kinetics of the leaching process was discussed. The results of this study suggest that pressure hydrochloric-acid selective leaching is a viable method for efficiently leaching Ni from laterite ores. (C) 2015 Elsevier B.V. All rights reserved.
机译:在这项研究中,基于为Fe-Si-Cl-H2O和Ni-Si-Cl-H2O系统构建的电位-pH图,使用加压盐酸选择性浸出从腐泥红土矿石中浸出Ni和Co。在各种条件下研究了镍,钴,镁,锰和铁的浸出。结果表明,在以下条件下可获得最佳产量:浸出温度为150℃,HCl浓度为350 g / L,液固比(I / s)为1.0,浸出时间为90分钟。通过X射线衍射分析,红外光谱和矿物释放分析来表征腐泥红土和浸出的残余物。根据结果​​分析了相关的酸浸出机理,并讨论了浸出过程的动力学。这项研究的结果表明,加压盐酸选择性浸出是一种有效地从红土矿石中浸出镍的可行方法。 (C)2015 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号