The effect of ceramic thickness and number of firings on the color of two all-ceramic systems.

机译:陶瓷厚度和烧成次数对两种全陶瓷系统颜色的影响。

获取原文
获取原文并翻译 | 示例
           

摘要

STATEMENT OF PROBLEM: All-ceramic restorations have been advocated for superior esthetics, and various materials have been used to improve ceramic core strength, but there is a lack of information on how color is affected by different core substructures and fabrication procedures. PURPOSE: The purpose of this study was to evaluate the effects of various dentin ceramic thicknesses and repeated firings on the color of lithium disilicate glass-ceramic (IPS e.max Press) and zirconium-oxide (DC-Zirkon) all-ceramic systems. MATERIAL AND METHODS: Thirty disc-shaped specimens, 4 mm in diameter with a 1-mm core thickness, and 0.5-, 1-, or 1.5-mm dentin ceramic thicknesses, were made from each of 2 ceramic systems (n=10). Repeated firings (3, 5, 7, or 9) were performed, and the color of the specimens was compared with the color after the initial firing. Color differences among ceramic specimens were measured using a spectrophotometer (VITA Easyshade), and data were expressed in CIELAB system coordinates. Repeated measures ANOVA was used to analyze the data (number of firings, ceramic composition, and ceramic thickness) for significant differences. The Tukey HSD test and paired 2-tailed tests were used to perform multiple comparisons (alpha=.05). RESULTS: L*a*b* values of the ceramic systems were affected by the number of firings (3, 5, 7, or 9 firings) (P<.001), ceramic composition (DC-Zirkon or IPS e.max Press) (P<.001), and ceramic thickness (0.5, 1, or 1.5 mm) (P<.001). Significant interactions were present in L*a*b* values between the number of firings and ceramic composition (P<.001) and between the number of firings and ceramic thickness (P<.001). Significant interactions were present between the number of firings and ceramic thickness and ceramic composition (P<.05) in L* and b* values, but not for the a* value (P=.068). As the ceramic thickness increased, significant reductions in L* values (P<.01) were recorded for IPS e.max Press and DC-Zirkon specimens. For IPS e.max Press specimens, there were significant increases in a* and b* values (P<.01). For DC-Zirkon specimens, significant increases in a* values were observed; however, no significant differences were recorded for b* values. CONCLUSIONS: The analysis revealed that there were significant changes in L*a*b* color data as the number of firings increased, which resulted in perceptual color changes in L*a*b* color parameters.
机译:问题陈述:提倡全陶瓷修复体具有卓越的美学效果,并且已使用各种材料来提高陶瓷芯的强度,但缺乏有关如何受不同的芯子结构和制造程序影响颜色的信息。目的:本研究的目的是评估各种牙本质陶瓷厚度和反复烧成对二硅酸锂玻璃陶瓷(IPS e.max Press)和氧化锆(DC-Zirkon)全陶瓷系统颜色的影响。材料与方法:用两个陶瓷系统(n = 10)分别制作三十个直径4毫米,芯厚1毫米,牙本质陶瓷厚度分别为0.5、1,或1.5毫米的圆盘形样品。 。重复烧制(3、5、7或9),并将样品的颜色与初始烧制后的颜色进行比较。使用分光光度计(VITA Easyshade)测量陶瓷样品之间的色差,并以CIELAB系统坐标表示数据。重复测量采用方差分析(ANOVA)分析数据(烧成次数,陶瓷成分和陶瓷厚度)之间的显着差异。使用Tukey HSD测试和成对的2尾测试进行多次比较(alpha = .05)。结果:陶瓷系统的L * a * b *值受烧成次数(3、5、7或9烧成)(P <.001),陶瓷成分(DC-Zirkon或IPS e.max Press)的影响)(P <.001)和陶瓷厚度(0.5、1或1.5 mm)(P <.001)。烧成次数和陶瓷组成之间的显着相互作用为L * a * b *值(P <.001),烧成次数和陶瓷厚度之间(P <.001)。在L *和b *值之间,烧成次数与陶瓷厚度和陶瓷组成(P <.05)之间存在显着的相互作用,但对于a *值则不存在显着相互作用(P = .068)。随着陶瓷厚度的增加,对于IPS e.max Press和DC-Zirkon标本,L *值明显降低(P <.01)。对于IPS e.max Press标本,a *和b *值显着增加(P <.01)。对于DC-Zirkon标本,观察到a *值显着增加。但是,b *值没有显着差异。结论:分析显示,随着发射次数的增加,L * a * b *颜色数据发生了显着变化,从而导致L * a * b *颜色参数的感知颜色发生了变化。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号