Assessment of protective properties of rubber lining in absorbers of flue gas desulphurization systems

机译:烟气脱硫系统吸收塔内衬的防护性能评估

获取原文
获取原文并翻译 | 示例
           

摘要

Results of research on degradation of rubber lining which is the main protection of absorbers in flue gas desulphurization (FGD) systems were presented. The power plant where the system operated is lignite-fired. Owing to measurements using electrochemical impedance spectroscopy and gravimetric determination of water content in the lining, the areas of the system which are most exposed to degradation were shown. The results obtained also allowed for optimization of protections used in absorbers, which resulted in lower density of lining at places with a lower risk of degradation. (C) 2014 Elsevier B.V. All rights reserved.
机译:提出了作为烟气脱硫(FGD)系统中吸收塔主要保护材料的橡胶衬里降解的研究结果。系统运行所在的发电厂是褐煤。由于使用电化学阻抗谱法进行的测量和衬里中水分含量的重量测定,显示了系统中最容易降解的区域。所获得的结果还可以优化吸收器中使用的防护装置,从而可以降低降解风险较低的地方的衬层密度。 (C)2014 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号