The synthesis of the thenoyltrifluoroacetone compound doped with terbium, dysprosium and europium encapsulated in a silica matrix (TTA:Tb:Dy:Eu@SiO_(2)) were performed by the sol-gel method. The precursors to obtain the vitreous phase (SiO_(2)) were: Tetraethylorthosilicate (TEOS, C_(8)H_(2)O_(4)Si, 98%, Aldrich), and ethyl alcohol (CH_(3)CH_(2)OH, 99.5%, Meyer), distilled water and 0.05 ml of hydrochloric acid (HCl, Meyer). The sample with molar ratio 20:80 TTA:Tb:Dy:Eu@SiO_(2) has the best emission intensity. Thermogravimetric analysis (TGA) shown that silica encapsulated samples decompose at lower temperatures than pure TTA:Tb:Dy:Eu luminescent material. Fourier Transform Infrared (IR-TF) shown the characteristic Si-O-Si bands that are presented at a wavelength of 1049, 853 and 440 cm~( &#45 1) confirming that the luminescent material is encapsulated in a silica matrix, finally X-ray diffraction (XRD) shown that TTA:Tb:Dy:Eu@SiO2 composite is amorphous.
机译:通过溶胶 - 凝胶法进行掺杂有铽,镝和铕的掺杂铽,镝和铕(TTA:Tb:Dy:Eu @ SiO_(2))的合成。获得玻璃体相的前体(SiO_(2))是:四乙酯硅酸盐(TEOS,C_(8)H_(2)O_(4)Si,98%,Aldrich)和乙醇(CH_(3)CH_(2 )哦,99.5%,梅白),蒸馏水和0.05ml盐酸(HCl,Meyer)。具有摩尔比例的样品20:80 TTA:Tb:Dy:Eu @ SiO_(2)具有最佳排放强度。图中分析(TGA)显示,二氧化硅包封样品比纯TTA:Tb:Dy:欧盟发光材料在较低温度下分解。傅里叶变换红外(IR-TF)示出了呈现在1049,853和440cm〜(&#451)的波长的特征Si-Si带,证实发光材料在二氧化硅基质中封装在二氧化硅基质中X射线衍射(XRD)显示TTA:Tb:Dy:Eu @ SiO2复合材料是无定形的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号