One of the Iranian copper deposits that is located east of Iran and also known as a primeval one in that area is Mesgaran Field. Old mining works have been clearly seen in the area. Iran is located on global copper belt and as a result it has numerous potential areas as copper deposits. The purpose of this study is identifying possible potentialities of copper mining in less developed regions of Iran with basic modern technologies. In this study, laboratory investigations of this field were done on samples via leaching and the cementation method. According to the study purposes, acid concentration, temperature, time and pulp density were selected as the main factors that were tested in leaching studies. Moreover, pH, temperature, time and the amount of iron powder were factors which were tested for copper cementation. Optimum conditions of leaching studies with 99.11% recovery rate were obtained after 120 grams per liter of H_(2)SO_(4), 80 degrees Celsius, 2 hours and 100 grams per liter of solid to liquid. On the other hand, optimum conditions of cementation by iron powder were resulted at more than 95% with a pH of 3, 45 degrees Celsius, 1 hour and 1.5 times more than the stoichiometric equation of required iron powder amount to precipitate copper.
机译:位于伊朗东部的伊朗铜矿床之一,也是该地区的原始矿床,是Mesgaran Field。该地区已经清楚地看到了古老的采矿工作。伊朗位于全球铜矿带上,因此它有许多潜在的铜矿床地区。这项研究的目的是通过基本的现代技术确定伊朗欠发达地区的铜矿开采潜力。在这项研究中,通过浸出和胶结法对样品进行了该领域的实验室研究。根据研究目的,选择酸浓度,温度,时间和纸浆密度作为浸出研究中测试的主要因素。而且,pH,温度,时间和铁粉的量是测试铜胶结的因素。 120克/升H_(2)SO_(4),80摄氏度,2小时和100克/升固体对液体后,可获得具有99.11%回收率的最佳浸出研究条件。另一方面,在pH为3、45摄氏度,1小时和1.5倍的条件下,通过铁粉进行胶结的最佳条件是沉淀铜所需的铁粉量的化学计量方程的95%以上。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号