Effect of Rejuvenator Containing Dodecyl Benzene Sulfonic Acid (DBSA) on Physical Properties, Chemical Components, Colloidal Structure and Micro-Morphology of Aged Bitumen

机译:十二烷基苯磺酸再生剂对老化沥青物理性质,化学成分,胶体结构和微观形貌的影响

获取原文
           

摘要

DBSA was used as a solubilizer together with conventional rejuvenator (CR) to produce a solubilized rejuvenator (SR), two kinds of aged bitumen involving TFOT aged bitumen and PAV aged bitumen were obtained by thin film oven test (TFOT) and pressurized aging vessel (PAV), respectively. Effects of CR and SR on the physical properties, chemical components, colloidal structure and micro-morphology of TFOT aged bitumen and PAV aged bitumen were investigated. Testing results of physical properties and chemical components indicated that CR and SR can replenish aged bitumen with necessary aromatics, TFOT aged bitumen that chemical component variation deteriorates its physical properties. With regard to PAV aged bitumen, of which the performance attenuation lies in chemical components variation and colloidal structure transformation, even if the content of CR reached up to 10 wt %, the regenerated bitumen cannot meet the regeneration requirement yet due to its definite influence on colloidal structure transformation, comparatively, sulfonic group in SR can react with the superficial atoms of asphaltenes to reform a solvation layer to facilitate the colloidal structure transformation of PAV aged bitumen, performance and beelike structure of regenerated PAV aged with bitumen with 10 wt % SR were approximated to that of virgin bitumen.
机译:DBSA与传统的再生剂(CR)一起用作增溶剂,生产增溶剂的再生剂(SR),通过薄膜烘箱试验(TFOT)和加压老化容器(TFOT)获得了两种老化的沥青,分别涉及TFOT老化的沥青和PAV老化的沥青( PAV)。研究了CR和SR对TFOT老化沥青和PAV老化沥青的物理性质,化学成分,胶体结构和微观形态的影响。物理性质和化学成分的测试结果表明,CR和SR可以为老化的沥青补充必要的芳族化合物,而TFOT老化的沥青则可以使化学成分的变化降低其物理性质。对于PAV老化沥青,其性能衰减在于化学成分的变化和胶体结构的转变,即使CR的含量达到10 wt%,再生沥青由于对沥青的确定性影响仍不能满足再生要求。胶体结构的转变,相比之下,SR中的磺酸基可以与沥青质的表面原子反应形成溶剂化层,以促进PAV老化沥青的胶体结构转变,再生的10%SR沥青的PAV的性能和蜂状结构分别为近似于原始沥青。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号