首页> 外文期刊>ZKG International >Method and system for producing low-alkalinity sulphoaluminate cement with new mineral system using steel slag
【24h】

Method and system for producing low-alkalinity sulphoaluminate cement with new mineral system using steel slag

机译:用钢渣用新型矿物系统生产低碱度硫铝酸盐水泥的方法和制备方法

获取原文
获取原文并翻译 | 示例
           

摘要

A method and system for producing low-alkalinity sulphoaluminate cement with a new mineral system using steel slag. The method includes the following steps: evenly mixing and homogenizing ground steel slag with dry desulfurization gypsum, aluminum ash and carbide slag according to a set ratio; and conveying the homogenized raw meal to a rotary kiln for calcination to obtain cement clinker, where the calcination temperature is 1200°C-1270°C, and the calcination time is 20-60 min; the alkalinity modulus of the homogenized cement raw meal is 0.81-0.9, and the Fe_2O_3 content is 8-13%. The method breaks through the requirements on contents of calcium, aluminum and iron in traditional sulphoaluminate cement production, and realizes application of a large amount of steel slag.
机译:一种用钢渣用新型矿物系统生产低碱度硫铝酸盐水泥的方法和系统。 该方法包括以下步骤:根据设定比例,具有干脱硫石膏,铝灰和硬质合金均匀混合和均化地钢渣; 并将均质原料膳食输送到旋转窑以获得水泥熟料,其中煅烧温度为1200℃-1270℃,煅烧时间为20-60分钟; 均质化水泥生膳的碱度模量为0.81-0.9,Fe_2O_3含量为8-13%。 该方法通过对传统硫代铝水泥生产中的钙,铝和铁含量的要求,实现了大量钢渣的应用。

著录项

  • 来源
    《ZKG International》 |2021年第5期|68-68|共1页
  • 作者

  • 作者单位
  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号