首页> 外文会议>China International Conference on High Performance Ceramics >Preparation and Microwave Dielectric Properties of (1-x)Ca_(2/5)Sm_(2/5)TiO_3-x Li_(1/2)Nd_(1/2)TiO_3 Ceramics
【24h】

Preparation and Microwave Dielectric Properties of (1-x)Ca_(2/5)Sm_(2/5)TiO_3-x Li_(1/2)Nd_(1/2)TiO_3 Ceramics

机译:(1-x)Ca_(2/5)Sm_(2/5)TiO_3-X Li_(1/2)ND_(1/2)TiO_3陶瓷(1/2)TiO_3陶瓷的制备和微波介电性能

获取原文

摘要

((1-x)Ca_(2/5)Sm_(2/5)TiO_3-x Li_(1/2)Nd_(1/2)TiO_3 (CSLNT) ceramics, suitable for use in resonators or filters at microwave frequency, have a high epsilon_r and a low temperature coefficient of resonant frequency. The effects of calcinations on the microwave dielectric properties of CSLNT were studied. The CSLNT (x = 0.3) ceramics sintered at 1300 deg C for 3 h showed microwave properties with epsilon_r of 92, Qf of 5060 GHz and tau_f of 7.5 ppm/ deg C. The microwave dielectric properties of CSLNT (x = 0.3) ceramics were also improved by soft chemistry methods such as citric acid gel route and ethylenediaminetetraacetic acid (EDTA) chelating method. The excellent microwave properties with epsilon_r= 96, Qf = 6290 GHz and tau_f- 6 ppm/ deg C were obtained by EDTA chelating method for CSLNT (x = 0.3) ceramics.
机译:((1-x)CA_(2/5)SM_(2/5)TIO_3-X LI_(1/2)ND_(1/2)TIO_3(CSLNT)陶瓷,适用于微波频率的谐振器或过滤器,具有高ε_R和低温谐振频率系数。研究了煅烧对CSLNT微波介电性质的影响。CSLNT(X = 0.3)陶瓷在1300℃下烧结3小时,显示微波性能92的EPSILON_R ,5060GHz和Tau_f的QF为7.5ppm / deg C.通过软化学方法如柠檬酸凝胶途径和乙二胺四乙酸(EDTA)螯合方法,还改善了CSLNT(X = 0.3)陶瓷的微波介电性能。优秀的通过EDTA Chelatic方法为CSLNT(X = 0.3)陶瓷,通过EDTA螯合方法获得微波性能= 96,QF = 6290GHz和Tau_F-6 PPM / DEG C.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号