Oil palm trunk is lignocellulose biomass and agricultural residual waste that has not been utilized to its maximum potential. The feasibility of paper production from oil palm trunk (OPT) was studied for one alternative application. OPT was treated with 8% (w/v) alkaline solution (NaOH), subsequently with a different concentration of H_2O_2 solution (2, 4, 6 and 8% w/v). The results showed that the brown color of OPP was converted to a pale yellow color after bleaching with H_2O_2 while hemicellulose and lignin were also removed. Arrowroot flour was used as a binder for mold oil palm paper. The optimum condition for oil palm paper production was 15% (w/v) NaOH for 60 min then 6 % (v/v) H_2O_2 for 30 min. The obtained OPP paper showed a density of 183.53 ± 1.86 g/cm~3, a water absorption of 0.0904 ± 0.0010 mL/cm~2, a tensile index of 2.60 ± 0.07 Nm/g and a burst index of 1.22 ± 0.04 kPa m~2/g. All value properties of the obtained OPP paper showed that the OPP value was lower than that of available commercial Kraft paper (KI125 and KT125). Meanwhile, this OPP paper process could continuously improve to be a container formation.
机译:油棕榈树干是木质纤维素生物量和农业残留废物,尚未用于其最大潜力。研究了来自油棕榈树干(OPT)的纸生产的可行性进行了一种替代应用。随后用8%(w / v)碱性溶液(NaOH)处理,随后具有不同浓度的H_2O_2溶液(2,4,6和8%w / v)。结果表明,在用H_2O_2漂白后,opp的棕色被转化为浅黄色,同时除去半纤维素和木质素。箭头粉用作模具油棕榈纸的粘合剂。油棕榈纸产量的最佳条件为60分钟的15%(w / v)NaOH,然后6%(v / v)H_2O_2持续30分钟。所得液体的密度显示为183.53±1.86g / cm〜3,吸水率为0.0904±0.0010ml / cm〜2,拉伸指数为2.60±0.07 nm / g,突发指数为1.22±0.04kPa m 〜2 / g。所得OPP论文的所有值特性表明,OPP值低于可用的商用牛皮纸(KI125和KT125)。同时,这种互换纸流程可能不断改进,成为容器形成。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号