Layer-structured Bi_5F_(0.5)Co_(0.5)Ti_3O_(15) Thin Films Grown by Pulsed Laser Deposition

机译:脉冲激光沉积生长的层状Bi_5F_(0.5)Co_(0.5)Ti_3O_(15)薄膜

获取原文

摘要

Layer-structured Bi_5F_(0.5)Co_(0.5)Ti_3O_(15), (BFCTO) ceramics exhibits a large magnetic moment increase of ~ 3 times by substituting half Fe by Co. The material has a four-layer unit cell, and presents a remarkable coexistence of ferroelectricity (FE) and ferromagnetism (FM) above room temperature (RT). The measured 2P_r and 2M_r are 13 μC/cm~2 and 7.8 memu/g, respectively, and the material's magnetic transition temperature is ~ 345 °C. This therefore raised an interest in further exploring the material's potential photonic applications when in thin films. In this research, an initial effort of thin film growth using the advanced pulsed laser deposition (PLD) approach was demonstrated. Such films' structural, morphological, and dielectric properties were studied.
机译:层结构的Bi_5F_(0.5)Co_(0.5)Ti_3O_(15),(BFCTO)陶瓷通过用Co代替一半的Fe表现出〜3倍的大磁矩增加。该材料具有四层晶胞,并呈现出室温(RT)以上的铁电(FE)和铁磁(FM)的显着共存。测得的2P_r和2M_r分别为13μC/ cm〜2和7.8 memu / g,材料的磁转变温度为345°C。因此,这引起了人们对进一步探索材料在薄膜中的潜在光子应用的兴趣。在这项研究中,证明了使用先进的脉冲激光沉积(PLD)方法进行薄膜生长的初步努力。研究了此类薄膜的结构,形态和介电性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号