SrTiO3 Functional Ceramics Thin Film Prepared by Self-Assembled Monolayers with the Liquid Phase Deposition Method on Silicon Substrates

机译:液相沉积法在硅基板上自组装单分子膜制备SrTiO3功能陶瓷薄膜

获取原文

摘要

In this article,(NH4)2TiF6,SrNO3 and H3BO3 were used as raw materials to prepare the precursor solution with the ratio ofAHFT/SN/BA=1∶1∶3.The thin films of SrTiO3 were fabricated on the functional silicon substrates (100) by self-assembled monolayers (SAMs) with the liquid phase deposition (LPD).This article also studied the effects of wet state and the deposition temperature of the precursor solution before and after the functionalization of silicon substrate on the thin film growth.The results indicated that after the immersion in OTS for 30min,the surface contact angle of the silicon substrate changed from 24.64° to 100.91°.The substrate appeared hydrophobic property and it was irradiated by UV light for 30min.Then the surface contact angle of the substrate decreased to 5.00°.The substrate appeared hydrophilicity.The concentration of the precursor solution was 0.025 mol/L,the deposition temperature was 40°C and the deposition time was 9h,which were all helpful to SrTiO3 crystallization.XRD and SEM were used to characterize the physical phase of thin film and surface morphology at 600 °C with annealing and heat retaining for 2h.The results indicated that the thin film prepared by the mono-crystal Si substrate was SrTiO3 thin film with better crystalline.On the crystal surfaces of (110),(100),(200) and (211),there appeared the obvious diffraction peaks.The SrTiO3 grains on the surface had the clear outline and were regular and long columnar crystals.
机译:本文以(NH4)2TiF6,SrNO3和H3BO3为原料制备比例为AHFT / SN / BA = 11:1∶3的前驱体溶液。 100)通过自组装单分子层(SAMs)进行液相沉积(LPD)。本文还研究了湿润状态和前驱溶液沉积温度对硅基板功能化前后薄膜生长的影响。结果表明,在OTS中浸泡30min后,硅基板的表面接触角从24.64°变为100.91°,基板呈现疏水性,并被紫外线照射30min。底物降到5.00°。底物呈现亲水性。前驱体溶液的浓度为0.025 mol / L,沉积温度为40°C,沉积时间为9h,均有利于SrTiO3的结晶。用XRD和SEM表征了薄膜的物相和表面形貌,并在600°C退火和保温2h,结果表明,单晶Si衬底制备的薄膜为SrTiO3薄膜。在(110),(100),(200)和(211)的晶体表面出现明显的衍射峰。表面的SrTiO3晶粒轮廓清晰,为规则长柱状晶体。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号