Provided is a method for producing a lithium cobalt phosphate represented by the following general formula (1):LixCo1-yMyPO4 (1), wherein 0.8≤x≤1.2 and 0≤y≤0.5, and M represents one or two or more metal elements selected from the group consisting of Mg, Zn, Cu, Fe, Cr, Mn, Ni, Al, B, Na, K, F, Cl, Br, I, Ca, Sr, Ba, Ti, Zr, Hf, Nb, Ta, Y, Yb, Si, S, Mo, W, V, Bi, Te, Pb, Ag, Cd, In, Sn, Sb, Ga, Ge, La, Ce, Nd, Sm, Eu, Tb, Dy, and Ho; the method comprising: a first step of adding an organic acid and cobalt hydroxide to a water solvent, and then adding phosphoric acid and lithium hydroxide thereto to prepare an aqueous raw material slurry (1); a second step of wet-pulverizing the aqueous raw material slurry (1) with a media mill to obtain a slurry (2) containing a pulverized product of raw materials; a third step of spray-drying the slurry (2) containing the pulverized product of raw materials to obtain a reaction precursor; and a fourth step of firing the reaction precursor. According to the present invention, a single-phase lithium cobalt phosphate in X-ray diffraction analysis can be obtained by an industrially advantageous method.
展开▼
机译:提供了一种制备由以下通式(1)表示的钴磷酸锂的方法:Li x sub> Co 1-y sub> m Y sub> PO 4 sub>(1),其中0.8≤x≤1.2和0≤y≤0.5,m表示选自Mg,Zn,Cu,Fe,Cr的一个或两个或多个金属元素。 ,Mn,Ni,Al,B,Na,K,F,Cl,Br,I,Ca,Sr,Ba,Ti,Zr,Hf,Nb,Ta,Y,Yb,Si,S,Mo,W,V ,Bi,Te,Pb,Ag,Cd,sn,sn,sb,ga,ge,la,ce,nd,sm,欧盟,tb,dy和ho;该方法包括:将有机酸和氢氧化钴加入水溶剂的第一步骤,然后加入其磷酸和氢氧化锂,以制备水性原料浆料(1);用介质研磨液湿法粉碎水性原料浆料(1)的第二步骤,得到含有原料粉碎产品的浆料(2);喷雾含有原料粉碎产物的浆料(2)的第三步,得到反应前体;和烧制反应前体的第四步。根据本发明,可以通过工业上有利的方法获得X射线衍射分析中的单相锂磷酸钴。
展开▼