0.5≤Cr+6Si+1.5W+11V+5Nb+10B−40C−30N−4Ni−2Co−2Mn≤10.0  (1)."/> Welding material for ferritic heat-resistant steel, welded joint for ferritic heat-resistant steel, and method for producing welded joint for ferritic heat-resistant steel
首页> 外国专利> Welding material for ferritic heat-resistant steel, welded joint for ferritic heat-resistant steel, and method for producing welded joint for ferritic heat-resistant steel

Welding material for ferritic heat-resistant steel, welded joint for ferritic heat-resistant steel, and method for producing welded joint for ferritic heat-resistant steel

机译:用于铁素体耐热钢的焊接材料,用于铁素体耐热钢的焊接接头,以及用于铁素体耐热钢的焊接接头的方法

摘要

The present invention provides a welding material for ferritic heat-resistant steel, a welded joint for ferritic heat-resistant steel, and a method for producing the welded joint for to form a weld metal having a high creep strength and a high toughness in welding a ferritic heat-resistant steel that contains B. The welding material for ferritic heat-resistant steel has a chemical composition containing, in mass %, C: 0.06 to 0.10%, Si: 0.1 to 0.4%, Mn: 0.3 to 0.7%, Co: 2.6 to 3.4%, Ni: 0.01 to 1.10%, Cr: 8.5 to 9.5%, W: 2.5 to 3.5%, Nb: 0.02 to 0.08%, V: 0.1 to 0.3%, Ta: 0.02 to 0.08%, B: 0.007 to 0.015%, N: 0.005 to 0.020%, with the balance being Fe and impurities, and satisfying Formula (1):0.5≤Cr+6Si+1.5W+11V+5Nb+10B−40C−30N−4Ni−2Co−2Mn≤10.0  (1).
机译:本发明提供了一种用于铁素体耐热钢的焊接材料,用于铁素体耐热钢的焊接接头,以及用于制造焊接接头的方法,用于形成具有高蠕变强度的焊接金属和焊接高韧性 含有B的铁素体耐热钢。用于铁素体耐热钢的焊接材料具有含有质量%,C:0.06至0.10%,Si:0.1至0.4%,Mn:0.3至0.7%的化学组合物的化学成分。 :2.6至3.4%,Ni:0.01至1.10%,Cr:8.5%至9.5%,W:2.5至3.5%,Nb:0.02至0.08%,V:0.1至0.3%,TA:0.02至0.08%,B: 0.007至0.015%,N:0.005至0.020%,平衡为Fe和杂质,并满足式(1): <?在线 - 公式描述=“线式公式”终止=“铅”?>0.5≤CR+ 6SI + 1.5W + 11V + 5NB + 10B-40C-30N-4NI-2CO-2MN≤10.0(1 )。<?在线 - 公式描述=“线式公式”终止=“尾”?>