首页> 外国专利> HIGH-WETTING LONG-CYCLE ALUMINA CERAMIC SLURRY AND PREPARATION METHOD THEREFOR, AND LITHIUM BATTERY DIAPHRAGM

HIGH-WETTING LONG-CYCLE ALUMINA CERAMIC SLURRY AND PREPARATION METHOD THEREFOR, AND LITHIUM BATTERY DIAPHRAGM

机译:高润湿的长循环氧化铝陶瓷浆料及其制备方法,锂电池隔膜

摘要

A high-wetting long-cycle alumina ceramic slurry and a preparation method therefor. The alumina ceramic slurry comprises the following raw materials: solid alumina, a dispersant, a wetter, a binder, a thickener, a defoamer, and pure water. The solid alumina comprises: high pore volume alumina and/or low pore diameter alumina; wherein the pore volume distribution of the high pore volume alumina is 0.4-3.0 ml/g, and the pore diameter distribution of the low pore diameter alumina is 0.1-5 nm. A lithium battery diaphragm comprises a PE film and the alumina ceramic slurry coated on the PE film. The use of the solid alumina greatly reduces the wetting time of the diaphragm and improves the production efficiency of batteries.
机译:一种高润湿的长循环氧化铝陶瓷浆料及其制备方法。氧化铝陶瓷浆料包括以下原料:固体氧化铝,分散剂,湿润剂,粘合剂,增稠剂,消泡剂和纯水。固体氧化铝包括:高孔体积氧化铝和/或低孔径氧化铝;其中高孔体积氧化铝的孔体积分布为0.4-3.0ml / g,低孔径氧化铝的孔径分布为0.1-5nm。锂电池隔膜包括PE膜和涂覆在PE膜上的氧化铝陶瓷浆料。使用固体氧化铝极大地减少了隔膜的润湿时间,提高了电池的生产效率。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号