451,774. Condensing metal vapours. ST. JOSEPH LEAD CO., 250, Park Avenue, New York, U.S.A. Feb. 11, 1935, No. 4364. Convention date, March 8, 1934. [Class 82 (i)] The vapours of volatile metals such as zinc, mercury, cadmium, magnesium, or tin are condensed by being drawn under vacuum through a bath of the liquid or molten metal which is agitated by the passage therethrough of the vapours, which are retarded by a series of baffles on the upper wall of an inclined condensing chamber. In the case, for example, of zinc, a bath of the molten metal in a chamber 1 is supplied with zinc vapour from a duct 2, and is subjected to a vacuum of 6 to 20 inches of mercury by a pump 4, so that the passage of the vapour agitates the molten metal, baffles 5 and 6 being provided to increase the agitation. The uncondensed gases such as CO are drawn off through chamber 3, washed in sprays 9, and collected in a gas holder 11. The temperature of the molten metal is maintained constant by pipes 12 in connection with a cooler 13, circulating pump 16 and furnace 14.
机译:451774。冷凝金属蒸气。 ST。约瑟夫铅公司(JOSEPH LEAD CO。),美国纽约公园大道250号,1935年2月11日,编号4364。会议日期为1934年3月8日。[第82(i)类]诸如锌,汞等易挥发金属的蒸气,镉,镁或锡是通过在真空下通过液态或熔融金属浴液而被冷凝的,而液态浴液或熔融金属浴液则通过蒸气的通过而被搅动,而蒸气通过倾斜的冷凝室上壁上的一系列挡板而受到阻碍。在例如锌的情况下,从导管2向腔室1中的熔融金属浴提供锌蒸气,并通过泵4对其施加6至20英寸汞柱的真空,使得蒸气的通过搅动了熔融金属,设置了挡板5和6以增加搅动。未冷凝的气体(例如CO)通过腔室3排出,在喷雾器9中清洗,并收集在储气罐11中。熔融金属的温度通过与冷却器13,循环泵16和炉相连的管道12保持恒定。 14。

著录项

  • 公开/公告号DE643363C

    专利类型

  • 公开/公告日1937-04-07

    原文格式PDF

  • 申请/专利权人 ST. JOSEPH LEAD COMPANY;

    申请/专利号DE1935ST53151D

  • 发明设计人

    申请日1935-02-19

  • 分类号C22B19/18;

  • 国家 DE

  • 入库时间 2022-08-24 05:48:29

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号