Pref. the difference between the two temps. is at least 30 degrees C. Pref. the temp. during half of moulding is 20 degrees above and in the remainder 10 degrees below vitrifying point. Pref. thermoplastics are polyesters, polyamides and terephthalic acid polyesters.
机译:首选两种温度之间的差异。至少为30摄氏度。温度在一半的成型过程中,玻璃化温度高出20度,其余的则低于玻璃化温度10度。首选热塑性塑料是聚酯,聚酰胺和对苯二甲酸聚酯。

著录项

  • 公开/公告号DE2300589A1

    专利类型

  • 公开/公告日1974-07-11

    原文格式PDF

  • 申请/专利权人 CHEMISCHE WERKE HUELS AG;

    申请/专利号DE19732300589

  • 发明设计人 IADAMUSHANSDR.;

    申请日1973-01-08

  • 分类号B29F1/08;

  • 国家 DE

  • 入库时间 2022-08-23 05:24:22

相似文献

  • 专利
  • 外文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号