A novel cracking catalyst, a method of preparing same and an improved hydrocarbon cracking process are provided wherein adverse effects of metals such as nickel, vanadium, iron, copper and cobalt in the cracking catalyst are precluded or mitigated by contacting the cracking catalyst with (A) at least one of elemental antimony and compounds thereof whereby there is added to said catalyst a modifying amount of each of (A) and (B) with the weight ratio of antimony to tin being such as to provide passivation of the contaminating metals greater than the sum of the passivation effects of each of (A) and (B) individually. In general the ratio will be in the range of from 0.001:1 to 1000:1, and preferably will be in the range of 0.05:1 to 50:1.
机译:提供了一种新颖的裂化催化剂,其制备方法和改进的烃裂化方法,其中通过使裂化催化剂与(A)接触来消除或减轻裂化催化剂中金属如镍,钒,铁,铜和钴的不利影响。 )元素锑及其化合物中的至少一种,从而将改性量的(A)和(B)中的每一种添加到所说的催化剂中,锑与锡的重量比使得钝化的污染金属大于(A)和(B)各自的钝化效果总和。通常,该比例将在0.001∶1至1000∶1的范围内,并且优选将在0.05∶1至50∶1的范围内。

著录项

  • 公开/公告号BR7806981A

    专利类型

  • 公开/公告日1979-05-08

    原文格式PDF

  • 申请/专利权人 PHILLIPS PETROLEUM CO;

    申请/专利号BR19787806981

  • 发明设计人 BERTUS B;MCKAY D;

    申请日1978-10-24

  • 分类号C10G11/02;B01J33/00;

  • 国家 BR

  • 入库时间 2022-08-22 20:50:51

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号