首页> 外国专利> SHOT PEENING SHOT AND RECOVERY METHOD OF SHOT

SHOT PEENING SHOT AND RECOVERY METHOD OF SHOT

机译:枪击事件和枪击的恢复方法

摘要

PURPOSE: To improve the recovery efficiency of shots by using as a shot for shot peening which is for giving residual compression stress to the surface of a material, a thing that has a specific grain diameter and is a magnetic body and is formed into an approximate spherical shape and is given with magnetism. ;CONSTITUTION: A shot peening shot is an object whose grain diameter is 0.3-1.2mm and which is a magnetic body and is formed into an approximate spherical shape and is given with magnetism, and is recovered by means of a brush jig having an electromagnetic magnet function. Also, the scattering of shots is restrained by providing an electromagnetic magnet at the bottom portion of a place where shots are scattered at the time of shot peening work. A shot such as above is manufactured into an approximate sherical shape by annealing ferrite stainless steel of a stick shape whose diameter is preferably 1.00mm, under the air condition of about 675-760°C and by conducting jetting against the wall of the same material by means of compressed air after having been cut off minutely into the ones whose lengths are about 1mm.;COPYRIGHT: (C)1995,JPO
机译:用途:为了提高喷丸的回收效率,将其用作喷丸处理的喷丸是为了向材料表面施加残余压缩应力,该喷丸具有特定的晶粒直径,是一种磁性体,形成为近似球形,并具有磁性。 ;组成:喷丸是一种粒径为0.3-1.2mm的物体,它是一种磁性体,形成为近似球形并具有磁性,并通过具有电磁性的电刷夹具进行回收。磁铁功能。另外,通过在喷丸处理时使散布的部位的底部设置电磁磁铁,来抑制散布的散布。通过在直径约675-760℃的空气条件下对直径优选为1.00mm的棒状铁素体不锈钢进行退火,并通过对相同材料的壁进行喷射,从而将上述丸粒制成近似于球形的形状。细切成长度约1mm的细丝后,用压缩空气吹制;版权所有:(C)1995,日本特许厅

著录项

  • 公开/公告号JPH07237125A

    专利类型

  • 公开/公告日1995-09-12

    原文格式PDF

  • 申请/专利权人 TOSHIBA CORP;

    申请/专利号JP19940029947

  • 发明设计人 OBATA MINORU;NAKAHIGASHI SHIGEO;

    申请日1994-02-28

  • 分类号B24C11/00;B24C1/10;B24C9/00;

  • 国家 JP

  • 入库时间 2022-08-22 04:26:20

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号