COATING LIQUID FOR FORMING COLORED FILM, COLORED FILM AND GLASS MATERIAL WITH COLORED FILM FORMED THEREON

机译:用于形成彩膜,彩膜和玻璃材料的彩涂液

摘要

PURPOSE: To obtain a coating liquid for forming a colored film aiming at the improvement of a tinting strength, heat resistant properties and the properties of preventing charged electricity by containing a liquid dispersed with a composite oxide pigment containing a specific element. ;CONSTITUTION: This coating fluid for forming a colored film is obtained by uniformly blending 1-90wt.% composite oxide pigment containing at least one element selected from Ti, V, Cr, Mn, Fe, Co, Ni, Cu and Zn and having 5-200nm average particle diameter, and as necessary, TiO2 containing nitrogen in a content of 0.1-30wt.%, a dispersing auxiliary agents such as a surfactant, a resin, an acid and an alkali, and water or an organic solvent to obtain the liquid for forming the colored film. A low resistance colored film reduced in light transmissivity in 380-700nm wave length range is obtained by coating the coating liquid on a transparent base substrate.;COPYRIGHT: (C)1996,JPO
机译:目的:获得一种用于形成着色膜的涂布液,其目的在于通过包含分散有包含特定元素的复合氧化物颜料的液体来提高着色强度,耐热性能和防止带电的性能。 ;组成:用于形成有色膜的涂布液是通过均匀混合1-90wt。%的复合氧化物颜料而获得的,该复合氧化物颜料包含至少一种选自Ti,V,Cr,Mn,Fe,Co,Ni,Cu和Zn的元素平均粒径为5-200nm,并且根据需要包含含量为0.1-30wt。%的氮,诸如表面活性剂,树脂,酸和碱的分散助剂的TiO 2 ,用水或有机溶剂获得用于形成着色膜的液体。通过将涂布液涂布在透明的基础基板上,得到在380-700nm的波长范围内的光透射率降低的低电阻的有色膜。COPYRIGHT:(C)1996,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号