MANUFACTURE OF NI-TI ALLOY SHEET AND NI-TI ALLOY MEMBER

机译:NI-TI合金板和NI-TI合金构件的制造

摘要

PROBLEM TO BE SOLVED: To manufacture an Ni-Ti alloy sheet capable of being rolled without causing edge crack, breaking or the like at the reduction ratio of 20-60% and to efficiently manufacture an Ni-Ti alloy member at a low cost. ;SOLUTION: (1) In this manufacturing method of the Ni-Ti alloy sheet by which a Ni-Ti base alloy is made into a sheet by applying rolling, a process constituted of annealing, grinding for making the surface roughness of both end faces in the width direction into ≤50m and cold rolling at a reduction ratio of 20-60% is executed one or more times. (2) In this method for manufacturing the Ni-Ti alloy member, the Ni-Ti alloy sheet is punched or cut so that it has partially the connecting parts, is subjected to the bending, then subjected to shape memory heat treatment without applying bending, thereby separating the connecting parts from the sheet.;COPYRIGHT: (C)1997,JPO
机译:解决的问题:制造能够以20-60%的压下率进行轧制而不会引起边缘裂纹,破裂等的Ni-Ti合金板,并以低成本有效地制造Ni-Ti合金构件。 ;解决方案:(1)在这种Ni-Ti合金薄板的制造方法中,通过施加轧制将Ni-Ti基合金制成薄板,该过程包括退火,磨削以使两个端面的表面粗糙度在宽度方向上≤50m,以20〜60%的压下率进行冷轧1次以上。 (2)在该Ni-Ti合金构件的制造方法中,将Ni-Ti合金板冲压或切割成具有部分连接部,进行弯曲,然后不施加弯曲地进行形状记忆热处理。 ,从而将连接件与板材分开。;版权:(C)1997,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号