The present invention mixes paper sludge with red mud or recycles red mud produced as a by-product from aluminum hydroxide manufacturing process to lightweight building materials or waste glass, waste pearl rock, waste diatomaceous earth, shell ( Specific gravity using a method in which a mixture of calcium carbonate-based waste), purified water, sewage sludge and coal ash, alone or in combination, is mixed in a suitable ratio in a temperature range of 900 ° C to 1200 ° C and a firing time within 10 minutes. It is to manufacture a porous red mud body having various specific gravity ranges between 0.6 and 2.5, and the red mud porous body manufactured as described above is used as a lightweight building material for light aggregate, soundproof panel, heat insulation or heat insulation panel.
机译:本发明将纸污泥与赤泥混合,或将由氢氧化铝制造过程中产生的副产物赤泥再循环到轻质建筑材料或废玻璃,废珍珠岩,废硅藻土,外壳(使用将碳酸钙基废物,纯净水,污水污泥和煤灰的混合物单独或组合以合适的比例在900°C至1200°C的温度范围内混合,并在10分钟内燃烧一次。要制造具有在0.6和2.5之间的各种比重范围的多孔红泥体,并且如上所述制造的红泥多孔体用作轻质建筑材料,用于轻骨料,隔音板,隔热或隔热板。

著录项

  • 公开/公告号KR100240943B1

    专利类型

  • 公开/公告日2000-03-02

    原文格式PDF

  • 申请/专利权人 NA CHOON-KI;LEE MU-SEONG;

    申请/专利号KR19980002478

  • 发明设计人 NA CHOON-KI;LEE MU-SEONG;

    申请日1998-01-30

  • 分类号C04B18/16;C04B18/24;

  • 国家 KR

  • 入库时间 2022-08-22 01:45:07

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号