ERBIUM AND YTTERBIUM IONS DOPED YTTERBIUM CALCIUM OXYBORATE COMPOUND, METHOD FOR GROWING CRYSTAL THEREOF, AND OPTICAL DEVICE PREPARED BY USING THE CRYSTAL

机译:掺AND硼酸RATE酸钙钙复合物,其晶体生长方法以及用该晶体制备的光学器件

摘要

PURPOSE: A crystalline solid material, a method for growing its crystal, an optical device prepared by using the crystal, and a method for preparing the optical device are provided, which solid material is erbium and ytterbium ions-doped ytterbium calcium oxyborate. CONSTITUTION: The crystalline solid material is represented by the formula: (Er(x)Yb(y)Y(1-x-y))Ca(4+z)B3O(10+z), wherein x is 0.005-0.10, y is 0.005-0.30 and z is 0.00-0.5. The crystal of the solid material is grown with the temperature gradient of 5-300 deg.C/cm by Czochralski method with the increasing velocity of 0.1-10mm/hr and the rotation velocity of 0-70 rpm. A YCa4O(BO3)3 crystal is used as a crystal seed. The solid material crystal is single crystal or thin film crystal. The optical device is a 1.5-1.6 micrometers laser generating device, a nonlinear optical device, a self frequency doubling device or a range finding device.
机译:目的:提供一种晶体固体材料,其晶体生长方法,使用该晶体制备的光学器件以及制备该光学器件的方法,该固体材料是和and离子掺杂的ions硼酸钙钙。组成:结晶固体材料由下式表示:(Er(x)Yb(y)Y(1-xy))Ca(4 + z)B3O(10 + z),其中x为0.005-0.10,y为0.005-0.30,z为0.00-0.5。固体材料的晶体通过Czochralski方法以5-300℃/ cm的温度梯度以0.1-10mm / hr的增加速度和0-70rpm的旋转速度生长。 YCa 4 O(BO 3)3晶体用作晶种。固体材料晶体是单晶或薄膜晶体。光学装置是1.5-1.6微米的激光发生装置,非线性光学装置,自倍频装置或测距装置。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号