首页> 外国专利> Surface-treated wood flour with physical reinforcing agent and vinyl chloride resin composition for the manufacture of synthetic wood with added wood flour

Surface-treated wood flour with physical reinforcing agent and vinyl chloride resin composition for the manufacture of synthetic wood with added wood flour

机译:具有物理增强剂和氯乙烯树脂组合物的表面处理木粉,用于添加木粉的合成木材的制造

摘要

The present invention improves the compatibility with the resin by treating the surface with a physical property enhancer in the wood powder used to manufacture synthetic wood to replace natural wood in a wide range of fields such as door frames, window frames, flooring, moldings, etc. It's about wood flour.;In addition, the present invention in the vinyl chloride resin composition used in the manufacture of synthetic wood, by adding wood powder to the vinyl chloride resin to give the extrusion molding the appearance and surface texture similar to natural wood, reducing the shrinkage rate during molding of the molded article and also in processability In addition to the vinyl chloride resin processing methods such as welding and bending, not only the wood processing methods such as planer and nailing can be processed, but also the wood powder in the resin during kneading by using wood powder treated with the physical property enhancer. To improve the dispersibility and flowability of the molten resin during extrusion, and to increase the mechanical properties such as tensile strength, flexural strength and impact resistance of the molded article. Wood gas and cup such as carbon monoxide (CO) and carbon dioxide (CO 2 ) This process eliminates the problem of corroding or shortening the life of extruding equipment by reducing wood gas, reducing the efficiency of extrusion molding, preventing surface roughness and pinhole phenomenon of extruded products, and easily corrupting molded products by residual moisture. The present invention relates to a vinyl chloride resin composition to which wood flour is added.
机译:本发明通过在门框,窗框,地板,装饰条等广泛领域中用物理性能增强剂处理用于制造合成木材的木粉替代天然木材来改善与树脂的相容性。此外,本发明用于制造合成木材的氯乙烯树脂组合物中,通过向氯乙烯树脂中加入木粉,使挤出成型的外观和表面纹理与天然木材相似。 ,降低模塑制品成型过程中的收缩率以及可加工性除了氯乙烯树脂加工方法(如焊接和弯曲)外,不仅可以加工刨床和钉子等木材加工方法,还可以加工木粉通过使用经过物理性能增强剂处理的木粉,可以在捏合过程中使树脂中的淀粉含量增加。为了提高熔融树脂在挤出过程中的分散性和流动性,并提高模制品的机械性能,例如拉伸强度,弯曲强度和耐冲击性。一氧化碳(CO)和二氧化碳(CO 2 )等木材气体和杯子通过减少木材气体,降低了挤出成型的效率,消除了腐蚀或缩短挤出设备寿命的问题,可防止挤出产品的表面粗糙和针孔现象,并容易因残留水分而破坏成型产品。本发明涉及添加木粉的氯乙烯树脂组合物。

著录项

  • 公开/公告号KR100301394B1

    专利类型

  • 公开/公告日2001-10-29

    原文格式PDF

  • 申请/专利权人 주식회사 엘지씨아이;

    申请/专利号KR19980056608

  • 发明设计人 임흥규;최덕순;

    申请日1998-12-21

  • 分类号C08L27/06;C08L25/08;C08L33/10;

  • 国家 KR

  • 入库时间 2022-08-22 01:12:09

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号