首页> 外国专利> Conducting of heat during metal inert gas or active gas welding for metallic materials esp. low-high alloyed steels and heat treated fine grain structural steel with a 0.2 percent yield strength or larger 900 N per mm2

Conducting of heat during metal inert gas or active gas welding for metallic materials esp. low-high alloyed steels and heat treated fine grain structural steel with a 0.2 percent yield strength or larger 900 N per mm2

机译:特别是在金属材料的惰性气体焊接或活性气体焊接过程中的导热。低-高合金钢和热处理的细晶粒结构钢,屈服强度为0.2%或每平方毫米900 N或更大

摘要

The heat conducting method is carried out so that the cooling off time of the welding seam is held during its range from 800 deg.C to 500 deg.C, carried out per root layer, per intermediate layer and per covering layer respectively 1 to 23 seconds.
机译:进行导热方法以使焊缝的冷却时间保持在其从800℃到500℃的范围内,分别对每个根层,每个中间层和每个覆盖层进行1到23秒。