PPROBLEM TO BE SOLVED: To provide a fine aggregate for cement concrete capable of providing a mortar or concrete having a good fluidity-retaining performance and useful in civil engineering and construction industries, and to provide a cement composition including the fine aggregate and also the cement concrete using the cement composition. PSOLUTION: This fine aggregate has a particle size of 0.1-5 mm, particularly includes 0.5% or more of a non-sulfate sulfur, is 20 mg/L or higher in concentration of the eluted non-sulfate sulfur, and further includes a blast furnace annealed slag, the glass content of which is 30% or less. The fine aggregate passes 100% through a sieve of 4.75 mm nominal dimension, 95-100% through 2.36 mm, 80-100% through 1.18 mm, 35-80% through 0.6 mm, 15-50% through 0.3 mm and 2-20% through 0.15 mm. The cement composition includes a cement and the above fine aggregate, and the cement concrete is composed by using the cement composition. PCOPYRIGHT: (C)2004,JPO
机译:

要解决的问题:提供一种用于水泥混凝土的细骨料,该细骨料能够提供具有良好的流动性保持性能并且在土木工程和建筑业中有用的砂浆或混凝土,并且提供一种包括该细骨料和水泥的水泥组合物。也使用水泥组合物的水泥混凝土。

解决方案:这种细骨料的粒径为0.1-5 mm,特别是含有0.5%或更多的非硫酸盐硫,洗脱的非硫酸盐硫的浓度为20 mg / L或更高,并且进一步包括玻璃含量为30%或更少的高炉退火炉渣。细骨料100%通过4.75毫米标称尺寸的筛子,95-100%通过2.36毫米,80-100%通过1.18毫米,35-80%通过0.6毫米,15-50%通过0.3毫米和2-20 %通过0.15毫米。所述水泥组合物包括水泥和上述细骨料,并且所述水泥混凝土通过使用所述水泥组合物来组成。

版权:(C)2004,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号