首页> 外国专利> Uranium foil having fine grains solidified rapidly from melt by cooling roll directly, and the fabrication apparatus and the fabrication process

Uranium foil having fine grains solidified rapidly from melt by cooling roll directly, and the fabrication apparatus and the fabrication process

机译:具有细晶粒的铀箔直接通过冷却辊从熔体中快速凝固,并且其制造设备和制造方法

摘要

The present invention is concerned with the fabrication process of low or high enrichment uranium and uranium alloy foil, and the fabrication apparatus therefor. Uranium (U) and uranium alloy ÄU-(A)Q-(B)X-(C)Y (Q: Al, Fe, Ni, Si, Cr, Zr element, X: Al, Fe, Ni, Si, Cr, Zr element, Y: Al, Fe, Ni, Si, Cr, Zr element, Q NOTEQUAL X NOTEQUAL Y, (A) ≤ 1 wt%, (B) ≤ 1 wt%, (C) ≤ 1 wt%)Ü foil are directly obtained from a melt, not through a vacuum induction melting & casting, ingot cutting, hot-rolling and heat-treatment process, but through melt spinning or a twin-roll casting process. Major advantages have been obtained as follows: 1) a simplified process without the hot-rolling process and heat-treatment process, 2) an improvement in productivity and process economics in foil fabrication, and 3) a high purity and a high quality of the foil.
机译:本发明涉及低或高浓缩铀和铀合金箔的制造方法及其制造设备。铀(U)和铀合金ÄU-(A)Q-(B)X-(C)Y(Q:Al,Fe,Ni,Si,Cr,Zr element,X:Al,Fe,Ni,Si,Cr ,Zr元素,Y:Al,Fe,Ni,Si,Cr,Zr元素,Q NOTEQUAL X NOTEQUAL Y,(A)≤ 1 wt%,(B)≤ 1 wt%,(C)≤ 1 wt%箔是直接从熔体中获得的,而不是通过真空感应熔铸,铸锭切割,热轧和热处理工艺,而是通过熔体纺丝或双辊铸造工艺获得的。获得了以下主要优点:1)简化了工艺,无需进行热轧工艺和热处理; 2)改善了箔片制造的生产率和工艺经济性; 3)高纯度和高质量的铝箔。挫败。

著录项

  • 公开/公告号KR100388808B1

    专利类型

  • 公开/公告日2003-06-25

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20000064237

  • 申请日2000-10-31

  • 分类号B21B1/00;

  • 国家 KR