首页> 外国专利> METHOD OF PRODUCING BAMBOO CHARCOAL, BAMBOO CHARCOAL, AND BAMBOO CHARCOAL-BLENDED SHEET

METHOD OF PRODUCING BAMBOO CHARCOAL, BAMBOO CHARCOAL, AND BAMBOO CHARCOAL-BLENDED SHEET

机译:竹炭,竹炭和竹炭混纺板的生产方法

摘要

PROBLEM TO BE SOLVED: To remarkably improve functions required for a bamboo charcoal product such as a far-infrared radiation function while making the most of its advantage.;SOLUTION: Raw material bamboo charcoal obtained by firing a bamboo material is refired at 500 to 1,200°C for 5 to 11 hr. Thus, the one having a resonant frequency of 0.5 to 5 Hz and an electric resistivity of 1 to 3 Ω cm can be obtained. A bamboo charcoal-blended sheet consisting of a foamed sheet of a synthetic resin blended with the fine powder of the bamboo charcoal having a mean particle diameter of 5 to 30 μm in the ratio of 10 to 50 wt.% can be produced.;COPYRIGHT: (C)2004,JPO&NCIPI
机译:解决的问题:在最大程度地发挥其优势的同时,显着改善竹炭产品所需的功能(例如远红外辐射功能);解决方案:将通过烧制竹材而获得的原料竹炭再烧成500至1200于5℃至11小时。因此,具有0.5至5Hz的谐振频率和1至3Ω的电阻率。厘米。可以生产由混合有合成树脂的泡沫片和平均粒径为5〜30μm的比例为10〜50重量%的竹炭细粉组成的竹炭混合片。 ;版权:(C)2004,JPO&NCIPI

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号