PROBLEM TO BE SOLVED: To provide a photocatalytic coating material excellent in transparency, hardness and decomposing performance and a method for producing the same and to provide a photocatalytic coated film having photocatalytic function obtained by coating the coating material.;SOLUTION: The photocatalytic coating material relates to improvement of the photocatalytic coating material containing titanium oxide powder and is characterized by the fact that the titanium oxide powder includes an anatase-type crystal structure wherein the interplanar spacing d value of the (101) plane of the anatase-type crystal obtained from the half-width of the diffraction peak of the (101) plane is 3.478 to 3.562Å. And the photocatalytic coating material comprises titanium oxide powder, aluminum oxide powder, a binder, a dispersing agent and a dispersant.;COPYRIGHT: (C)2004,JPO
机译:解决的问题:提供透明性,硬度和分解性能优异的光催化涂料及​​其制造方法,并提供通过涂布该涂料而获得的具有光催化功能的光催化涂膜。本发明涉及含有二氧化钛粉末的光催化涂料的改良,其特征在于,二氧化钛粉末具有锐钛矿型晶体结构,其中,锐钛矿型晶体的(101)面的面间距d值由下式获得: (101)面的衍射峰的半峰宽为3.478〜3.562&。并且该光催化涂料包括氧化钛粉末,氧化铝粉末,粘合剂,分散剂和分散剂。;版权所有:(C)2004,日本特许厅

著录项

  • 公开/公告号JP2004143453A

    专利类型

  • 公开/公告日2004-05-20

    原文格式PDF

  • 申请/专利权人 MITSUBISHI MATERIALS CORP;

    申请/专利号JP20030342902

  • 申请日2003-10-01

  • 分类号C09D201/00;B01J35/02;B32B9/00;C09D5/00;C09D5/14;C09D5/16;C09D7/12;

  • 国家 JP

  • 入库时间 2022-08-21 23:34:34

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号